Partsframes, paddles, boards, poles
Surfaceweave set in the outer fabric
Sized byflex curve first, then lay-up
The floorallowable strain, not ultimate strength
A sports part is not an industrial part with a different drawing. An industrial part fails and the line stops. A sports part fails and the rider comes off the bike, the paddler goes over into the water. So this work needs three things at once — light, durable, good-looking — plus one that is never negotiable: it does not fail.
Carbon fibre sports and outdoor parts, made to drawing. Moulds are cut by a partner toolmaker to our specification and we sign them off; cost and ownership are agreed per project.
Custom parts to drawing Carbon fibre tube Moulding processes
Light: the grams are the selling point
In this trade weight is not a parameter; it is the selling point. Take 100 g off a frame and it can move up a price band. Take 20 g off a paddle and an hour on the water feels different.
Light costs stiffness. Carbon takes the weight out. How much it can take depends on the load: pedalling runs between the bottom bracket and the head tube. The stroke runs through the transition from shaft to blade, and the lay-up in those two places is not the same.
So grams and flex curve are set together — curve first, then lay-up. A quote that names a weight and no curve will be felt by the rider on the first ride.
Durable: ten thousand cycles, not one pull to break
Sports parts take repeated load. A frame sees a few thousand pedal cycles in a single ride, a paddle goes through hundreds of strokes an hour, a snowboard bends tens of thousands of times in a season.
Fatigue and static strength are different questions. A part that passes statically can still fail in fatigue, and fatigue starts where stress concentrates — at joints, at hole edges. The wall steps in thickness. The same holds for industrial parts; only here the cycle counts are higher and the loads less tidy.
Two more things count outdoors: UV and salt spray. Yellowing resistance in the clearcoat, corrosion protection on the metal parts — both sit under outdoor exposure.
E-bike frames: one more layer, and it is electrical
An e-bike frame carries a layer the frame itself does not. The battery compartment has to be sealed, flame retardant and insulated. No one material does all three: flame retardance comes from the resin formulation, insulation from keeping the carbon away from anything live. Sealing from the groove. The choice splits at material selection — it cannot be added at assembly.
Looks: the visible face is the product
On a sports part the visible face is the product. Weave, clearcoat, colour: the customer looks at that layer before anything else.
Weave is set in the outer fabric, not added afterwards. Plain is tight and even; twill has direction and follows compound curvature better. At the same weave, 3K and 12K differ in tow size, and the surface reads at a different grain. Forged carbon has no direction at all — it comes from the way the charge flowed in the mould.
The clearcoat has to take abrasion. We recommend it on exposed faces, but scratches show more on a natural finish than on paint, so edges want protecting through transport and assembly.
Colour goes two ways: natural plus clearcoat, where you see the fibre; or paint, where you see the colour master. If it has to line up with the rest of the product, the colour master is made together with it.
The floor: when it breaks, someone gets hurt
The trade mostly does not write this down, and it is the real barrier in it.
Metal bends before it breaks, and the bend can be felt. A composite has no yield point: it moves very little before it goes, and feel is a poor guide. So sports parts are designed to allowable strain rather than to ultimate strength, with a further safety factor on anything that sits close to the body.
Three things follow in process: reinforcement at joints and hole edges, a retained sample from every batch, NDT on the critical parts. Hole edges and the area around inserts are the default fatigue origins — that is where the reinforcement goes. Skip the three and the price comes down a step, and the risk moves to the user.
Testing and responsibility
This trade has public test outlines, and the buyer wants part-level evidence, not "we do it well".
The outline follows the part: frames sit in the ISO 4210 / EN 14781 family, helmets in the EN 1078 family. Part-level validation runs at enquiry and sampling stage. The report goes with the parts with the data listed item by item — a test report, not a certification. Not a signature on the customer's behalf.
The boundary, stated plainly: we make the part and run the part-level validation. Whole-vehicle approval and whole-helmet type examination are filed by the customer. A helmet is PPE; type examination goes through a Notified Body, and that step is not ours.
What we do not take on
- No whole-product assembly — no complete bikes, no complete sets of equipment.
- No secondary machining on customer-supplied parts. Machining is for the parts we moulded; that is where the responsibility stops.
FAQ
Can you make a few samples first?
Yes. First-off runs on soft tooling to prove shape, weight and feel; the mould goes to steel when volume arrives.
Can a frame be built to our geometry?
Yes — to drawing or to a geometry table. The difficulty in a frame is not the moulding; it is the lay-up, and the reinforcement at two interfaces: the bottom bracket and the head tube.
How close can the weight be held?
Per part. At a given shape, weight and bending stiffness are a pair: fix the stiffness first, then the weight. The other way round does not work.
Can the weave be specified?
Yes — plain, twill, 3K, 12K, forged carbon. On curved parts it is confirmed against a sample panel; clearcoat comes in gloss and matt.
Can you run to outlines like EN 14781?
Part-level validation to the outline, yes, and the report comes with it. The approval is filed by the customer; we do not sign it on their behalf.
How long does it take?
Lead time is agreed per project: sampling and series run on separate schedules, with the mould, the production slot and inspection each taking their own time. Both are given with the quote.
How are UV and salt spray handled?
A clearcoat chosen for yellowing resistance, and corrosion protection on the metal parts. For long outdoor exposure we suggest an ageing comparison at sample stage.
Who cuts the mould, and who owns it?
A partner toolmaker cuts it to our specification and we sign it off. Cost and ownership are agreed per project.
Give us the geometry and the weight target, and the lay-up follows; give the weight alone and the lay-up is guesswork.
Request a quote