Carbon and glass fibre profiles: L, C, T, I and flat bar, section to drawing, ±0.1 mm, cut to length. For frames, rails, panel stiffening and structural ties.

Carbon fibre flat bar

ProfilesCarbon fibre

Width 5–50 mm, thickness 0.5–10 mm, section 2.5–500 mm² (width-to-thickness 2:1–100:1; outside that, square bar or sheet)

Pultrusion, unidirectional 0°

Carbon fibre angle

ProfilesCarbon fibre

Equal leg 10×10–100×100 mm (80 and above made to drawing), wall 1–10 mm

Pultrusion

Carbon fibre channel

ProfilesCarbon fibre

Channel depth 20–150 mm, flange width 10–75 mm, wall thickness 1.5–6 mm

Pultrusion

Carbon fibre I beam

ProfilesCarbon fibre

Section depth 30–200 mm, flange width 20–120 mm, wall thickness 2.5–8 mm

Pultrusion

Carbon fibre T profile

ProfilesCarbon fibre

Section depth 20–150 mm, flange width 20–100 mm, wall thickness 2–6 mm

Pultrusion

GRP angle

ProfilesGlass fibre

Equal leg 25–150 mm, wall 3–12 mm; unequal leg to drawing

Pultrusion

GRP channel

ProfilesGlass fibre

Height 50–200 mm, width 25–75 mm, wall 3–12 mm

Pultrusion

GRP I beam

ProfilesGlass fibre

Depth 60–300 mm, flange 30–150 mm, wall 4–12 mm

Pultrusion

Not in the list?

Made to drawing

Send the drawing or the duty — we will say whether it can be made, and how.

Talk to us

The section comes from the die — change one dimension and it is a new die

L, C, T, I and flat bar are all pultruded, and the section is formed by the die. Which is why profiles suit a design that has settled and will run for a while. While the shape is still moving, build it from plate or tube and cut the die once the form is fixed. Shaped sections with ribs, grooves or unequal walls are possible, but the demould and the fibre path have to be assessed first.

How it arrives

Cutting to length, drilling and end machining are in house. Long sections ship in a wooden crate with edge protection, so a visible face arrives unmarked.

What a quotation needs

A section drawing or the dimensions including wall, plus length, quantity and load direction. If the section is still moving, send the target and we will say which dimensions force a new die.

Send the drawing. We will send the route.

A drawing, a photo of a failed part, or three lines of requirement is enough to start. Scope, price indication and lead time within 24 hours.

No commitment · NDA available · Reply within 24 hours

Request a quote WhatsApp