Rigid carbon fibre sheet
PlatesCarbon fibre
Thickness 0.3–50 mm; full sheet 2440×1220 mm (4×8 ft)
Compression moulding (continuous fibre) / (chopped, forged finish); pultruded UD to drawing
PlatesCarbon fibre
Thickness 0.3–50 mm; full sheet 2440×1220 mm (4×8 ft)
Compression moulding (continuous fibre) / (chopped, forged finish); pultruded UD to drawing
PlatesCarbon fibre
Overall thickness 6–30 mm; skin 0.5–1.5 mm (0.75 mm minimum below 8 mm overall); core 4–27 mm
Adhesive-film hot pressing, vacuum bagging, WCM wet compression moulding
PlatesGlass fibre
Thickness 0.5–50 mm; full sheet 1220×2440 mm or 1020×1220 mm
Hot-pressed lamination; continuous lamination for thin sheet, compression moulding for thick
Made to drawing
Send the drawing or the duty — we will say whether it can be made, and how.
Talk to us
Load-bearing faces take solid laminate: thickness holds ±0.05–0.2 mm and flatness 0.3 mm/m. Where stiffness has to come with low weight, use a sandwich panel — skins and core are formed in one shot, not bonded afterwards. Solid sheet suits end plates, flanges, base plates and machined parts; sandwich suits large covers and hatches with few supports.
Full sheets are 2440×1220 mm. Cutting, nesting, drilling, edge milling and filming are all in house. Nesting follows your layout, and the material yield is stated on the quotation rather than charged as an extra.
Thickness, sheet size, quantity, surface (one face or both, gloss or matte) and whether it needs film. Send a nesting drawing if you have one and the cut price is worked from it.
A drawing, a photo of a failed part, or three lines of requirement is enough to start. Scope, price indication and lead time within 24 hours.
No commitment · NDA available · Reply within 24 hours