Vehicle lightweighting

Composite parts are expensive in the tooling and cheap at volume — provided the line is there.

Partsbody structure, outer panels, chassis, enclosures

ProcessesHP-RTM / moulding / winding / pultrusion / LFT-D

Volumesoft tooling for first-off, steel for series

Mouldscut to our spec by a partner, signed off by us

Composite parts are expensive in the tooling and cheap at volume — that does not hold at most composite plants: the labour sits in the lay-up. Volume never spreads it. Our answer is to hand the lay-up to equipment — the preform is cut automatically and laid layer by layer by robot; on the HP-RTM line, closing, injection, cure and demoulding all run inside the line, and the only people in it are loading, unloading and inspecting. Down to 3–5 min a shot, with the parameters logged shot by shot. The larger the volume, the better that line pays.

Both small batches and large. Small batches start on soft tooling to get shape, fit-up and the vehicle interface working; as volume arrives the mould goes to steel and the part moves onto the HP-RTM line. Moulds are cut by a partner toolmaker to our specification, and we sign them off; cost and ownership are agreed per project. Moulding and finishing sit in the same plant — five process lines, chosen by part, none of them by default.

Body structure, outer panels, chassis and driveline, interior and exterior trim — all four run on this site. Part type is not the limit: a door today, a battery tray tomorrow, on the same line. The thinking does not change — fix the load path and the assembly first, then the process and where the mould splits.

Cheap at volume — if the line is there

The same part, with annual demand an order of magnitude apart, wants a different process.

At the small-batch stage the mould is soft and the work is getting shape. Fit-up and the vehicle interface right by hand — labour is a large share of the piece price, and that tuition cannot be skipped. As volume arrives, the mould goes to steel and the part goes onto HP-RTM: preform cut automatically and laid robotically, with injection weight. Mould temperature and cure time held by the machine, so the only labour inside the line is load, unload, inspect. That is where the cost curve turns down.

So the move that matters at volume is changing the line, not squeezing the supplier. Leave the line where it is and every point taken off the price comes back through quality.

Cheap at volume comes in two kinds. Pultrusion is priced by the metre and gets cheaper as the run lengthens: what it saves is material and mould — near-net shape, little scrap, one die per section. HP-RTM saves labour and spreads the mould: 3–5 min a shot. Both are friends of volume; they save on different items in the quote.

What will not come down at volume is hand lay-up and vacuum bagging: the labour is all in the lay-up. Volume spreads the mould but not the hours. Winding sits in another bracket — the machine winds, people load and unload the mandrel; it comes down with volume, but not to HP-RTM levels. Those parts run on a different pricing logic; do not apply HP-RTM arithmetic to them.

Three more things are just as unavoidable in series production: mould life, batch consistency, and the tolerance stack that lets the part fit the vehicle. Mould life sets the amortisation, consistency sets the scrap rate, the stack decides whether it goes on the car. All three go into the quote; none of them can be added after series start.

Body parts, by position

Structural parts — body load paths, chassis mounts, battery and underbody protection, seat frames. Designed to the load path and the crash path. Composites do not fold plastically the way steel does, so crash behaviour is carried by simulation and by part-level rig testing — drop weight, crush — all in our own plant, not estimated from experience and not sent out; full-vehicle crash testing runs on the customer's programme. HP-RTM or compression moulding, with metal inserts moulded in. The hard part is not the weight saved; it is keeping the original mounting points, load paths and service removal sequence.

Stress plot of a boom-lift arm
Stress plot of a boom-lift arm: the peak sits at the highest bending moment, which is where the material grade steps up.

Outer panels — bonnet, door skins, wings, spoilers. Designed to surface. Class A comes from the mould face, the lay-up sequence and the resin content, not from sanding; a sanded panel shows waves in the light.

Chassis and driveline — driveshafts, leaf springs, suspension parts. These are moving parts, where fatigue and balance outrank static strength; more on that below.

Interior and exterior trim — trim parts and clad parts. Moulded to a forged-carbon or twill surface with the clearcoat exposed and no paint; where the colour has to match the interior, it goes to paint or to cladding.

Carbon fibre trim part with ribs inside the opening
Clearcoat and twill outside; ribs and opening formed in one shot.

Once a vehicle is in series, documents and systems run to the project: material certificates, batch traceability, first-article report, dimensional report. Anything not on that list is said before the quote, not written into a promise.

Wheels: the one-piece part is possible

We make one-piece carbon wheels — and not just the cosmetic face.

The difficulty in a wheel is not the moulding; it is the validation: radial fatigue, bending fatigue and impact, all three. Testing runs to the outline the customer supplies, with the parameters set by the wheel's load rating, not carried over from another wheel.

On process, a wheel is a classic HP-RTM or compression moulded part: fibre oriented along the spoke load path. The bolt-hole area thickened with a metal insert moulded in. Balance starts in the mould — concentricity and a symmetric lay-up hold the imbalance down — and what remains goes through conventional balancing.

The approval route follows the market the customer sells into: a one-piece carbon wheel for road use has to clear something like TÜV or ECE R124 first. We supply the parts and the test samples; the approval is filed by the customer or by a nominated body. A project with no approval path stops at the track and the show car.

Battery enclosures: four requirements at once

The battery tray and enclosure is the hardest part on this page: it has to carry load, be flame retardant, keep water out. Not conduct.

Those four are not four operations. They are fixed by one material choice and one structural design:

Flame retardance comes from the resin system, not from the fibre type — carbon parts use a flame-retardant resin too. Glass fibre is there for non-conduction: wherever isolation is needed, glass goes in. No direct path is left between the carbon and a live part inside the enclosure. Sealing comes from the groove and the locating feature, fixed at moulding like the shell itself, not from a gasket fitted afterwards. Load comes from inserts and ribs, calculated against the customer's crush and vibration cases.

Targets are verified to the customer's standard; we do not set numbers of our own. Enclosure crash and crush follow the customer's whole-vehicle case, with the simulation and the part-level testing both in our hands.

Thermal runaway is a separate layer. It has to be split out at concept stage: fire protection belongs to the customer's pack design — mica sheet, intumescent coating. Venting and pressure relief. What the enclosure gives is flame-retardant substrate and structural load; it does not replace the pack's thermal management.

Trucks and trailers: tare weight is payload

The arithmetic on a trailer is not the arithmetic on a car. On a car, weight saved buys fuel and range. On a trailer it converts straight into payload: less tare weight is more freight on every trip, and that money is counted per trip, not per year.

Trailer panels — pultruded plank or sandwich panel. Pultruded plank resists corrosion and needs no paint, and stands up to moisture and road salt; sandwich is lighter, but the joint between panels has to be engineered — rivet, adhesive or profile clip, and the wrong choice works loose within six months. The joint is settled at quote stage, not at fitting.

Leaf springs — glass fibre for most, carbon-glass hybrid where it has to be lighter. A steel leaf spring rusts and its rate changes with it; a composite one does not, and that is the real advantage, beyond the weight. Three things decide whether it can be a direct replacement: the rate curve has to line up, the mounting points are carried over, the suspension geometry does not move. Miss one and the suspension comes with it.

Load-bearing sections — side rails, cross members, post sections. Constant section and long: pultrusion is the cheapest route — the die is cut to the section, and a change of size is a change of die.

None of these sits in an OEM programme. The customer is a trailer builder, a converter or a special-purpose vehicle maker, and the questions are piece price, lead time and whether it lasts.

Driveshafts: rotating parts are another account

A driveshaft is one of the few rotating parts on a vehicle, and it is engineered on quite different lines from a static structure.

First, critical speed. The longer and thinner the shaft, the lower the first critical speed. Carbon's specific stiffness pushes it up at the same length, but how far has to be calculated, not estimated.

Second, balance. Wall thickness consistency in winding and fibre tension consistency decide the imbalance directly. A perfect tube on off-centre flanges is worth nothing.

Third, the joint. Metal flange to composite tube is adhesive plus mechanical fastening: torque goes through the adhesive, the fasteners only stop peel. Bond area, surface preparation and cure temperature in that joint test the process harder than the tube does.

Failure looks different too: a steel shaft shakes before it goes, a composite one delaminates, and there may be no warning before the shake. So driveshaft validation is rig-based, not proven by fitting it to a vehicle.

Outer panels: four traps

Pinholes. A moulded surface has micro-voids, and paint straight onto it blisters. Either the mould face is taken further, or a sealing primer goes on — the second is less work on the mould and one more operation at the end.

Colour. Matching steel body colour needs the same colour master and the same paint batch. Composite reads dark underneath, so a light colour will not cover it; a hiding layer goes on first.

Carbon fibre bonnet, three-quarter view showing weave and highlight
Surface from mould and lay-up; the highlight shows if it was sanded.

Thermal expansion. A large panel moves in sunlight, so the fixing points need room for it; they cannot be locked to steel tolerances.

Paint bake. This is the one that most often goes wrong. An outer panel entering an OEM paint line meets e-coat and topcoat bakes at 160–180 °C; most epoxy systems have a glass transition temperature of 120–150 °C, so the part goes over temperature on the way in and comes out with all three at once — distortion, blistering, orange peel. Either the system changes to a high-Tg one, or painting moves off-line at low temperature, and that is settled before the quote, not discovered at the oven.

What we do not take on

No whole-vehicle assembly, no electronic controls.

No secondary machining on customer-supplied parts. Machining is for the parts we moulded; that is where the responsibility stops.

Parts we have made

Boom lift arm

Special-purpose vehicle: material graded by bending moment — high-strength steel at the root section, carbon and steel hybrid through the middle sections, plain carbon only at the smallest tip section; the boom went from 22 m to 29 m and the whole arm came out 100 kg lighter.

FAQ

Do you take small batches as well as large ones?

Both, with the process split between them. Small batches are proved on soft tooling first and move to steel as volume arrives; the two price differently, so the mould cost and the piece price have to be read together.

What cycle can a series part run at?

By part and by process. Compression moulding and HP-RTM are an order of magnitude apart, and LFT-D is another bracket again. The cycle is quoted together with the mould cost; the piece price is not quoted on its own.

Who cuts the mould, and who owns it?

A partner toolmaker cuts it to our specification and we sign it off. Cost and ownership are agreed per project; at volume the mould can be amortised into the piece price.

Do you make one-piece carbon wheels?

Yes. Radial fatigue, bending fatigue and impact run to the customer's test outline, with parameters set by the wheel's load rating.

Will a composite leaf spring replace a steel one directly?

The rate curve has to line up, the mounting points carry over, and the suspension geometry must not change. All three, or the suspension comes with it.

Can an outer panel match the body colour?

Yes, with the same colour master and a hiding layer — and the bake temperature has to be checked: for an OEM paint line, the resin system is chosen to the bake.

Give us the CAD and the annual volume, and process and mould are choices you can make.

Request a quote

sales@atomfrp.com WhatsApp +853 68617664

Send the drawing. We will send the route.

A drawing, a photo of a failed part, or three lines of requirement is enough to start. Scope, price indication and lead time within 24 hours.