Where the money goes

The first line of a buyer’s email is usually “how much for this part”. Honestly: a carbon fibre part is not sold by weight. It is five bills stacked, and which bill dominates depends on the part, not on the material. Give the size, the quantity and the duty, and you get a range within 24 hours. All five bills are settled inside our plant — nothing is subcontracted.

Why a price per kilo is always wrong

Same sheet, cut into ten brackets. Then cut into a thousand. The material in each bracket does not change, yet the unit price can differ several times over — and the difference is not material. It is tooling spread over ten parts or a thousand, plus the handling, lay-up and demoulding that repeat for every single part, whatever the batch size. A price per kilo prices the sheet. It says nothing about what the sheet became.

The five bills What it is How it moves with volume
Material Fibre, resin, consumables — and the part of the sheet cut away Fixed per part; follows the blank, not the batch
Tooling Mould, fixtures, trimming jigs One-off; divided by the number of parts
Labour Lay-up, vacuum, closing, cure, demoulding Per part; falls only when the cycle changes
Finishing Cutting, drilling, edge sealing, painting, bonding, assembly Per feature and per surface requirement
Inspection Dimensions, appearance, batch records Per batch; export adds a document set

Material: the share falls as the part gets smaller

On a large, simple flat panel, material is the biggest share of the unit price: a big blank, cut fast, little work after it. Shrink the part and the same sheet yields more pieces an hour; material’s share drops and labour and finishing rise. That is why price per kilo only sounds reasonable on large parts. On a bracket it counts the sheet and not the work done to it.

At low volume and one-off, the work sets the price, not the material — that is the route custom parts take.

One more layer: material is costed on the blank, not on the finished part. Nesting, edge allowance and offcuts all sit in that line. A badly nested shape can add a visible slice to the material bill.

Tooling: a one-off that decides whether small batches are expensive

On most quotations this is the largest single line. The tool is bought once and divided by the number of parts: ten parts carry the whole tool, a thousand parts share it. Small batches are expensive here. Late drawing changes also hurt here — change the structure after the tool is cut and the tool may be scrap. So change early, and change once.

There is one way to save it: before the tool is cut, settle the mounting face, the parting line and the draft angle. Once.

Labour: the only line a production line compresses

Hand lay-up, vacuum, closing, cure, demoulding — that loop runs for every part. Automation compresses this line, provided the shape was designed for a press cycle. A shape that insists on being laid by hand will not come down. On the quotation this line follows the cycle, not the drawing.

The difficulty here is not speed but consistency: a stable cycle is what makes a price stay put.

Finishing: where the part becomes a product

Cutting, drilling, edge sealing, painting, inserts, assembly. This is not the largest line — tooling is — but it adds most to the unit price: every hole, every edge that has to be masked, every bonded insert needs a pair of hands, and any of them can scrap the part at the last step. A part with nothing to drill and nothing to paint is cheaper than it looks.

Inspection: a small line, a hard gate

Dimensions, appearance, and the record that ties the part to its fibre and resin batch. Export orders usually add a document set. It is small on the quotation and large on the schedule: nothing ships without passing, and a failure goes back through the queue.

When no honest number exists

Miss any one of three and there is no honest number: structure undecided, duty unstated, quantity unknown. With all three, you get a range, a lead time and a suggested process route within 24 hours — that is how the order process runs.

What to send

How big the part is, how many, and what duty it has to carry. We can ask the rest; without these three the price is a guess.

For choosing the process, see Pultruded or roll-wrapped tube.

Need a manufacturability review? Start an RFQ