A carbon fibre centre console trim is judged by how it looks in the car, not by a coupon. This one runs on HP-RTM at twelve cavities, eight minutes a cycle, and the visible face comes out of the tool.
Constraint
The customer supplied a drawing: the outer face of a centre console trim has to be the carbon weave itself — the same weave, the same gloss, part after part — at 40,000 a year. Hand finishing at that rate is not a plan. The surface has to come out of the tool.

Solution
HP-RTM. A dry preform is loaded into a 12-cavity tool, resin is injected under pressure, and the part cures in the mould. The visible face is formed against the polished tool surface, so the weave and the gloss are set by the tool rather than by a finisher.
Result
300 g a part; 12 cavities on an 8-minute cycle, 90 parts an hour; a 30-day tool. The year's 40,000 parts ran in 23 days. Part geometry and the customer name are withheld under NDA; the photograph shows the packing, not the part.
Parts outside the standard catalogue are made to drawing, on the same tooling and inspection route. Send the drawing and you get a route, a tolerance and a lead time.