Carbon and glass fibre plate: laminate 0.3–50 mm, thickness ±0.05–0.2 mm, flatness 0.3 mm/m, moulded up to 2440×3650 mm. 3K twill on one or both faces, filmed or cut and nested to drawing.

Fibreglass sheet

PlatesGlass fibre

Thickness 0.5–50 mm; full sheet 1220×2440 mm or 1020×1220 mm

Hot-pressed lamination; continuous lamination for thin sheet, compression moulding for thick

Not in the list?

Made to drawing

Send the drawing or the duty — we will say whether it can be made, and how.

Talk to us

Thickness and layup decide whether it is a plate or a shell

Load-bearing faces take solid laminate: thickness holds ±0.05–0.2 mm and flatness 0.3 mm/m. Where stiffness has to come with low weight, use a sandwich panel — skins and core are formed in one shot, not bonded afterwards. Solid sheet suits end plates, flanges, base plates and machined parts; sandwich suits large covers and hatches with few supports.

How it arrives

Full sheets are 2440×1220 mm. Cutting, nesting, drilling, edge milling and filming are all in house. Nesting follows your layout, and the material yield is stated on the quotation rather than charged as an extra.

What a quotation needs

Thickness, sheet size, quantity, surface (one face or both, gloss or matte) and whether it needs film. Send a nesting drawing if you have one and the cut price is worked from it.

Send the drawing. We will send the route.

A drawing, a photo of a failed part, or three lines of requirement is enough to start. Scope, price indication and lead time within 24 hours.