Overview

Fibreglass sheet is laminated, not cast. Layers of glass cloth are stacked, saturated with resin and cured under temperature and pressure. Thickness comes from the ply count, and the cut edge shows cloth, layer after layer, that decides two things. The sheet is the same density from face to core. A thick sheet is not thin sheets glued together, it is pressed in one operation. Resin you choose affects the result more than which thickness does: change the resin at the same thickness and strength, temperature. Water absorption and unit price all have to be read again. For how to choose, see "Choosing between epoxy, polyurethane and polyester" below. For insulation, read the resin first and the thickness second. Breakdown voltage is not linear in thickness, twice the thickness is not twice the withstand. Choose on a multiple of the working voltage rather than calculating against the limit. The standard sheet sizes are 1220×2440 mm, which is 4×8 ft, and 1020×1220 mm, which is 40×48 in. Both are matched to presses, moulds and logistics and are the general laminate sizes. Anything outside them is scheduled to drawing, machining is done in house. Water-jet guided laser for outlines and holes, CNC for profiling, counterbores and edges, grinding where the thickness has to be tight, nesting from a DXF. Glass fibre wears tooling faster than carbon fibre. That shows up in the machining charge, not in the tolerance. A dry laser is not used. It chars the resin and melts the glass into balls, but a water-jet guided laser cuts it cleanly. The same profile can be supplied as a machined part: custom composite parts.

Request a quote

Environment and properties

Dielectric properties: high volume resistivity, more stable in damp conditions than polyester systems, which suits high-voltage insulating supports and barriers.

Chemical resistance: resists acids, alkalis and most solvents; check the specific medium against concentration and temperature, and confirm strongly oxidising media separately.

Low water absorption: the epoxy system absorbs the least, so electrical performance moves least under permanent humidity or immersion.

Non-magnetic: non-metallic and non-magnetic, so it can be used for non-metallic supports and locating parts on MRI equipment.

Low thermal expansion: dimensionally stable through temperature change, which suits parts that mate with metal components.

No rust: a non-metallic matrix that does not oxidise or rust, and needs no coating to keep it that way.

Where it is used

  • Electrical insulation: insulating shim, transformer and switchgear supports, terminal boards, busbar barriers
  • Tooling and jigs: equipment base plates, test frames, probe supports, assembly fixtures
  • Machinery and equipment: wear pads, guide strips, machinery blocks, guard plates
  • Electronics assembly: insulating dividers, non-metallic supports
  • Anti-corrosion linings: chemical plant liner plates, laboratory bench tops

Stock sizes in detail

Areal weight calculated at a density of 2.0 g/cm³; thickness tolerance banded to IEC 60893-2.

Thickness mm Tolerance mm kg/m² Typical use
0.5 ±0.12 1.00 Insulating shim, divider
1.0 ±0.18 2.00 Shim, cover plate
1.5 ±0.24 3.00 Shim, cover plate
2.0 ±0.28 4.00 Divider, guard plate
3.0 ±0.37 6.00 Equipment base plate, insulating support
4.0 ±0.45 8.00 Equipment base plate, tooling substrate
5.0 ±0.52 10.00 Tooling substrate, shim plate
6.0 ±0.60 12.00 Structural shim, wear plate
8.0 ±0.72 16.00 Load-bearing shim
10 ±0.82 20.00 Load-bearing shim, mould shim
12 ±0.94 24.00 Heavy-duty shim
15 ±1.10 30.00 Heavy-duty shim
20 ±1.30 40.00 Machinery block
25 ±1.50 50.00 Machinery block
30 ±1.70 60.00 Large block
40 ±2.10 80.00 Heavy block
50 ±2.45 100.00 Heavy block

Choosing between epoxy, polyurethane and polyester

Choosing a resin is not choosing the expensive one; it is choosing the right one. Ask the following in order and the answer falls out. Will it sit in water or permanent damp? If so, epoxy first. Epoxy has the lowest water absorption, and after immersion its dimensions and electrical performance degrade least. Polyester loses dielectric performance noticeably once it has absorbed water, so an insulating part needs a larger margin. Will it be hit, bent or shocked? If so, polyurethane first. Polyurethane is the tougher of the three, with better impact and bending resistance at the same thickness. Suits guard plates, shim plates and structural parts carrying assembly stress. Epoxy is hard and brittle and cracks readily at a sharp corner. Is the budget tight? If so, unsaturated polyester. Polyester has the lowest unit price and enough resistance to acids, alkalis and most solvents for general insulating shim. Equipment liner and tooling base plate work. The price is more shrinkage, flatness on thick sheet one band worse, and strength one band lower, the dividing line in one sentence. insulation and dimensional stability, epoxy, toughness and impact resistance, polyurethane, cost and general purpose, polyester.

Thickness sets the ply count. The ply count is the thickness A sheet does not get thicker by pressing harder. The thickness comes from the number of plies, each cloth adding one increment, so the thicknesses available step rather than run continuously. Thin sheet (0.5–3 mm) takes its thickness from the layup, holds a tight tolerance, and can be ground to ±0.05 mm. This band is for shims, dividers and insulating pieces where thickness matters, so the quotation should state "nominal thickness plus tolerance" plainly. Medium sheet (3–15 mm) is the most used band: equipment base plates, insulating supports, tooling substrates, test frames. Flatness here comes from the mould and the press, not from grinding afterwards. Thick sheet (15–50 mm) has to be ground on both faces. Unground, the middle bulges slightly and it will not pull flat at assembly. Thick sheet is priced by weight rather than by area, because the resin and cloth are all inside it,

Insulation: the resin. The thickness. | The insulating performance of glass sheet comes from the volume resistivity of the resin. From the absence of a conducting path between cloth layers. Epoxy is best, polyurethane next, polyester enough in dry conditions. In damp conditions the gap widens, water molecules reach between the layers, and polyester's dielectric loss rises fastest. Thickness and withstand voltage are not linear. Double the thickness and the breakdown voltage does not double, because a thicker sheet has a higher probability of internal defect. Size on a multiple of the working voltage; do not force it onto a "so many millimetres per so many volts" table. Breakdown voltage and volume resistivity. No figures are quoted for now, only "selected by resin system and thickness, testing available on request". Figures go in once the tests have been run.

Post-machining: done in house, arrives as a part

A full sheet is nested from a DXF and water-jet cut to size. The water-jet guided laser cuts outlines and holes, CNC mills the edge, counterbores and notches. Anything needing a tighter thickness goes to grinding. It goes straight into packing; you do not run it through another operation. Cutting: the water-jet guided laser cuts outlines and holes with a small heat-affected zone and no burning or breakout, outline ±0.1 mm. Thick sheet can also be water-jet cut and then CNC-trimmed. Sawn to ±2 mm, CNC-milled edge ±0.2 mm. Holes and slots: hole position ±0.01 mm; counterbores, steps, notches and chamfers to drawing. Edge distance from three hole diameters, four is safer, glass bearing strength is low, and a short edge tears at assembly. It is checked against the drawing at nesting. Grinding: a full sheet to ±0.25 mm, a small piece to ±0.05 mm. From 15 mm up the sheet is supplied ground on both faces, so it pulls flat at assembly, Threads: the sheet is not tapped. Interlaminar shear will not hold a thread, and repeated assembly strips it. Threaded parts take a metal insert or a through bolt with washers, fitted in house. Sealing: a cut edge exposes fibre and water travels along it. Parts for outdoor, damp or chemical service are sealed in house, with resin of the same system or an end cap. Glass fibre wears tooling faster than carbon fibre, and both tool consumption and cycle time are higher. That shows up in the machining charge rather than the tolerance.

Sheet size and cutting

The 1220×2440 mm sheet is made to 4×8 ft and the 1020×1220 mm to 40×48 in. These are the general laminate sizes, with presses, moulds and logistics all built around them. The point of full-sheet cutting is one joint fewer. A two-metre equipment base plate needs two or three joints if it is made from small sheets. Every joint is a break in stiffness and in appearance. Cut from a full sheet there is no such break. Send a DXF layout and we place the parts on one sheet, with offcuts still yielding small parts, quoted as sheet price plus machining. A full sheet ships in a wooden crate and freight is by volume. Cut to the layout first and the volume comes down, with the freight behind it.

Colour and surface

Colour depends on the resin. Epoxy's natural colour is pale green, jade green in the trade, and that is what it is without pigment. Polyester and polyurethane can be pigmented, with yellow, black, green and white the common options, and pigmenting carries a minimum order. The surface is either gloss or matte. Pressed against steel plate the gloss is flat enough for a visible face. Pressed against release film the matte carries a fine texture and needs no abrading before bonding. Where a thinner sheet or a tighter thickness is needed, it goes to grinding. Grinding is charged per piece: a full sheet to ±0.25 mm, a small piece to ±0.05 mm.

Delivery states

  • Full sheet Supplied at standard sheet size, protective film intact
  • Cut Cut to drawing or to a nested layout, size tolerance ±2 mm
  • Precision cut CNC milled edge, size tolerance ±0.2 mm
  • Ground Thickness ground to a specified value, ±0.05 mm on a small piece; from 15 mm up the full sheet is supplied this way — it does not ship unground
  • Machined part Drilled, slotted, counterbored, chamfered, to drawing
  • Assembly Combined with metal parts and inserts, batch production after first-article approval

Tolerance and inspection

Length and width (sawn) ±2 mm ±2 mm
Length and width (CNC) ±0.2 mm ±0.2 mm
Diagonal difference 2 mm/m of diagonal 0.5 mm/m of diagonal
Flatness IEC 60893-2 bands 0.3 mm/m after grinding
Thickness after grinding ±0.25 mm (full sheet) ±0.05 mm (small piece only)
Edge Sawn edge CNC-milled edge, chamfered

Common questions

What resin does the sheet use?

Epoxy, polyurethane or unsaturated polyester. Epoxy has the best strength and dimensional stability and the lowest water absorption. Polyurethane is the tougher and more impact-resistant. Polyester is the cheapest and the most general-purpose

How do I choose between epoxy, polyurethane and polyester?

Permanent water contact or insulation: epoxy, impact and bending: polyurethane. Tight budget, general insulation and chemical resistance: polyester. Strength and temperature are not the same band across the three, so each system is quoted separately

What thicknesses can you make?

0.5 mm to 50 mm, in steps. Thin sheet takes its thickness from the layup; thick sheet is ground on both faces. Thicknesses outside the table are quoted to drawing

What is the thickness tolerance?

Banded to IEC 60893-2, from ±0.12 mm on thin sheet to ±2.45 mm at 50 mm, step by step in the tolerance table. Anything tighter goes to grinding, which reaches ±0.05 mm on a small piece

What is the largest sheet?

A full sheet of 1220×2440 mm (4×8 ft) or 1020×1220 mm (40×48 in). Sheet size does not change with thickness, both run across the whole range. Sizes outside these are scheduled to drawing

Can it be laser cut?

Yes, with a water-jet guided laser: no charring and no breakout, outline ±0.1 mm and hole position ±0.01 mm. A dry laser is not used, because it chars the resin and melts the glass into balls

Can it be tapped?

Not advisable straight into the sheet. The interlaminar shear strength will not hold a thread, and repeated assembly strips it. Use a bonded metal insert, or a through bolt with washers

What does post-machining cover?

Water-jet guided cutting, CNC milling, drilling, slotting, counterbores, chamfers, grinding and edge sealing, all in house. A drawing or a DXF is enough

How do I tell an epoxy sheet from a polyester one?

Colour is only a guess: epoxy is pale green naturally, polyester is commonly yellow, green or black. The reliable way is the cut edge and the water absorption, or asking the supplier for the resin system. We cannot judge someone else's sheet on colour alone

Is there a flame-retardant grade?

The standard sheet is not flame retardant. UL94 V-0 is required it is made to a flame-retardant formulation and sent for testing. With the standard and acceptance criteria stated at order and the report issued per batch. The flame-retardant version is a separate formulation with its own quotation and its own scheduling. A standard sheet cannot be sent for flame-retardant certification

Are G10 and FR4 the same thing?

No. The standard sheet is G10, which is not flame retardant. FR4 is a different formulation with flame retardant added and carries a UL94 V-0 rating. Mechanical and electrical performance are close, but the flame rating is not interchangeable. V-0 is required the order has to go on the flame-retardant grade

Can you make insulating parts?

Yes. Insulation depends on the resin system and the thickness: epoxy best, polyurethane next, polyester enough in dry conditions, damp conditions need margin. Electrical testing can be provided on request

Can I choose the colour?

Epoxy is pale green naturally and stays that colour uncoloured. Polyester and polyurethane can be pigmented, with a minimum order

Will it absorb water and move?

Epoxy, polyurethane and polyester all absorb little; epoxy the least. In permanent immersion or high humidity, epoxy's dimensions and electrical performance degrade least

Can you make a sandwich construction?

Yes. Thin sheet either side of a core, made to drawing, for a larger sheet and less weight

What are the MOQ and lead time?

Full sheets in standard sizes start at one sheet; cut and machined parts are quoted per piece. Stock availability and lead time for standard sizes depends on capacity at the time, and non-standard thicknesses are scheduled

Send us the size

Section, length, quantity and service conditions — with these in hand the quote is accurate. Upload a drawing if you have one; without one, the same figures written out will do.

No file selected

PDF, DWG, DXF, STEP, STL, ZIP or a phone photo — up to 20 MB.

The part, the material, the size — or the problem it has to solve. Drawings and photos can go in the field above.

+ Company, quantity, timeline

Used only to answer this enquiry and for related technical follow-up.

  • Company address Zhuyuan Tianhuan International, No. 76 Keji 2nd Road, High-tech Zone, Xi'an, Shaanxi, China
  • Factory Fengjing Industrial Park, Middle Section of Fengwu East Road, Huyi District, Xi'an, Shaanxi, China
  • Sales email sales@atomfrp.com
  • Phone (WeChat) +86 18191567691 Email and forms answered 24/7; phone Mon–Fri 09:00–18:00 GMT+8
  • WhatsApp +853 68617664 Email and forms answered 24/7; phone Mon–Fri 09:00–18:00 GMT+8
  • A named engineer replies within 24 hours
  • NDA can be signed before any file is sent
  • Drawings and requirements are not disclosed

Send the drawing. We will send the route.

A drawing, a photo of a failed part, or three lines of requirement is enough to start. Scope, price indication and lead time within 24 hours.

No commitment · NDA available · Reply within 24 hours