Overview

Carbon fibre sandwich panel. Two thin carbon fibre skins with a light core between them. Honeycomb cores, aramid paper, PP, aluminium, are for ultra-light large panels; foam cores, PMI and PVC, for load-bearing and temperature duty. Overall thickness 6–30 mm, skin 0.5–1.5 mm, stock panel 1220×2440 mm, the core holds the skins apart. Flexural stiffness rises with the square of that separation while weight rises only with core density. A 20 mm panel with 1 mm skins and a PMI core is 4.18 kg/m². Against 31 kg/m² for a solid carbon sheet of the same thickness. Overall tolerance ±0.3 mm, flatness 1.5 mm/m. Weight per square metre is in the table, so the weight and freight of a full panel can be worked out directly. Outside the standard range, the same section is made as a part to drawing: see custom composite parts.

Request a quote

Where it is used

  • Load-bearing faces for equipment enclosures and covers
  • Tops and treads for mobile platforms
  • Vehicle panels, partitions and door panels
  • Cleanroom wall and ceiling panels
  • Building partitions and rainscreen backing panels
  • Large panels for exhibition stands, props and temporary structures

Stock sizes in detail

Read it as overall thickness − skin − core. Areal weight follows the build: at the same thickness, changing the core can double the weight.

Code Overall Skin Core Core density Areal weight (nominal, ex-film) kg/m² Note
SW-06-075-PVC 6 0.75 PVC foam 80 2.69 Light partition
SW-10-05-PVC 10 0.5 PVC foam 80 2.27 Enclosure panel
SW-10-10-PVC 10 1.0 PVC foam 80 3.74 General panel
SW-15-10-PVC 15 1.0 PVC foam 80 4.14 Worktop and partition
SW-20-10-PVC 20 1.0 PVC foam 80 4.54 Vehicle panel
SW-25-10-PVC 25 1.0 PVC foam 80 4.94 Load-bearing floor
SW-30-15-PVC 30 1.5 PVC foam 80 6.81 Heavy-duty tread
SW-15-10-PMI 15 1.0 PMI foam 60 3.88 Thin skin, high stiffness
SW-20-10-PMI 20 1.0 PMI foam 60 4.18 Light load-bearing panel
SW-20-15-PMI 20 1.5 PMI foam 60 5.67 Point-load resistant
SW-15-10-AFH 15 1.0 Aramid honeycomb 64 3.93 Large panel
SW-20-10-AFH 20 1.0 Aramid honeycomb 64 4.25 Large load-bearing panel
SW-20-10-PPH 20 1.0 PP honeycomb 80 4.54 Cost first
SW-10-05-ALH 10 0.5 Aluminium honeycomb 50 2.00 Ultra-light enclosure
SW-20-10-ALH 20 1.0 Aluminium honeycomb 72 4.40 Load-bearing, needs isolation layer

Overall thickness, skin thickness, core thickness

The trade writes 20-1.0-PMI60: 20 overall, 1.0 skin, PMI core, core density 60 kg/m³. Overall thickness decides bending. Sandwich bending comes almost entirely from how far apart the two skins are; the core itself does not bend. On a panel with 1.0 skins and a PMI 60 core, taking overall thickness from 10 to 20 mm raises flexural stiffness about four times. Areal weight goes only from 3.58 to 4.18 kg/m², up 17%. The extra is the core alone. Not a gram has been added to the skins. This is the thing that makes a sandwich panel pay: thickness is nearly free. Skin thickness decides tension, compression and impact. Too thin and local load dents it first. A footstep leaves a dent. Thicker and areal weight climbs steeply, because carbon fibre is twenty times the density of the core. At 0.5 mm the skin suits only panels over 10 mm overall that see pure bending and no point load. At 6 mm overall the skin is not below 0.75 mm. Anything thinner will not hold a weave and will dent under a point load first. That build leaves a 4.5 mm core. The sandwich effect is deliberately weak here. This is a light partition and enclosure sheet, with the skins doing the bending; it is not a load-bearing panel. For load, start at 15 mm. 1.0 mm is the general-purpose figure; 1.5 mm and above is for foot traffic, pressure or impact. Core thickness = overall − 2 × skin. It sets the distance between the skins, and whether the core can stand up on its own. Too thin, under 4 mm, and the sandwich effect is not there, and a solid sheet would be the better answer. The three dimensions are not chosen independently: overall thickness sets stiffness, skin sets point-load resistance, core sets weight and cost. The combinations in the table are built in that order.

Where the money goes in a sandwich

A sandwich panel is skins, core and adhesive film, and each has one job. The skins carry bending and impact. One skin in tension, one in compression, forming a couple. The fibre in the skin runs along the main bending direction, exactly as in a solid sheet. The core holds the skins apart. It carries almost no bending stress. What it carries is shear, all the slip between the two skins goes through it. That makes the core's shear strength more critical than its compressive strength. It is the most commonly missed point: most people look only at core density, and high density does not mean high shear strength. The adhesive film holds the two together. The bond line between skin and core is the thinnest layer in the structure and the most underrated. In a badly bonded panel the skins peel away from the core in bending and stiffness falls off a cliff, nothing shows on the surface. It only feels soft when you press it. So choosing a sandwich is not choosing "the lightest core": it is "a core with enough shear, an adhesive that holds. A skin thick enough to take point load". Miss one and the other two are wasted money.

Core selection: honeycomb and foam core

Each core has its place, and the densities in the table are the usual bands rather than the whole range.

CoreDensity kg/m³Flatwise compressionShearTemperatureSuitsDoes not suit
PMI foam50–110highhighhigh (to 180 °C)thin skins, high stiffness, hot pressing, temperature dutytight budgets, thick panels
PVC foam60–200medium-highmedium-highmedium (about 80 °C)general structural panels, balance of cost and performancehigh-temperature cure, long-term heat
Aramid honeycomb48–80mediummediummedium-highlarge area, ultra-light, secondary structureconcentrated point load, local bearing
PP honeycomb70–120mediummediummedium (about 100 °C)low cost, impact resistance, recyclableheat, high-stiffness duty
Aluminium honeycomb40–85medium-highhighhighultra-light, large area, high stiffness, temperatureneeds thermal isolation. In contact with carbon fibre an isolation layer is required, or damp conditions cause galvanic corrosion
One trap : honeycomb has high flatwise compression strength but thin cell walls. A screw crushes them straight away. To fix anything to a honeycomb panel, bury a solid block or potting compound in the core first. Without it the bolt will not tighten, and vibration will loosen it. Foam cores are better but still will not take high torque. Every fixing point in a sandwich panel needs designing separately. If you are unsure: bending-led and light, PMI or aramid honeycomb. Fixing, foot traffic, screws. A thicker skin on PVC foam with the fixing points designed in. Cost first and indoor duty, PP honeycomb.

Edge sealing

A cut sandwich panel has an open section. Exposed core at the cut edge. That is not an appearance problem, it is a durability problem. Why it has to be sealed: foam and honeycomb are open-cell, so moisture goes in at the cut edge and does not come out. A damp panel does not fail immediately, but it gains weight, freezing drives the skins apart, and the bond line degrades. In a dry indoor environment dust sealing is enough; outdoors, in damp conditions or where the panel is washed, it has to be sealed. Pick the seal by the application:

  • Adhesive seal: a structural adhesive brushed on the cut edge, or an adhesive-film edge tape — the lightest form of bonding. Thinnest and quickest. Right for indoor, dry, non-structural edges.
  • Bonded-in frame: place timber, aluminium profile or composite strip where the core will be cut, before cutting. The cut edge is solid. For edges that will be drilled, jointed or loaded. The most expensive and the most reliable.
  • Edge wrapping: the same material or an aluminium profile wrapped round the edge and bonded under pressure. For exposed edges where appearance matters.
Decide it at cutting. Edge sealing is part of the process rather than a later operation, once the panel is cut, adhesive sealing is all that is left. For a bonded-in frame, draw the frame position on the drawing and we place it at layup.

Areal weight against a solid sheet of the same thickness

Areal weight, weight per square metre, is the number to look at on a sandwich panel. It decides how heavy the panel is, what the freight costs and how many people lift it. The sum is simple: the two skins plus the core.

areal weight kg/m² = 2 × skin thickness (mm) × 1.55 + core thickness (mm) × core density (kg/m³) ÷ 1000
Some rows from the table, side by side:
  • 20 mm / skin 1.0 / PMI 60: 4.18 kg/m², against 31.0 kg/m² for a solid carbon sheet of the same thickness — 87% lighter
  • 20 mm / skin 1.0 / aramid honeycomb 64: 4.25 kg/m², 86% lighter
  • 30 mm / skin 1.5 / PVC 80: 6.81 kg/m², against 46.5 kg/m² solid — 85% lighter
But lighter is not the whole story. At the same thickness a solid sheet is stiffer in bending, because the whole section is working. The comparison that matters is which is lighter at equal stiffness:
  • 20 mm sandwich, skin 1.0: second moment of area about 180 mm⁴/mm of width, areal weight 4.18 — stiffness per kilogram 43
  • 20 mm solid sheet: about 667 mm⁴/mm, areal weight 31.0 — stiffness per kilogram 21.5
In other words, to match a 20 mm solid sheet the sandwich has to go to about 37 mm, at roughly 5.2 kg/m². The 20 mm solid sheet is 31 kg/m². At equal stiffness a sandwich panel is usually about a sixth of the solid weight, and the lighter the core the lower that fraction. The other way round. If the space is fixed and the panel can only be 3 mm thick, a sandwich buys nothing. A solid sheet is the right answer.

Length, cutting and ends

Stock panel 1220×2440 mm, also available at 1000×2000. Larger is cut to drawing, limited by sheet and press size. Cutting. CNC milling is the usual route, leaving a clean edge and cutting notches and rebates in the same pass. Water-jet does not chip a thin panel, but a sandwich section contains core, and the jet scorches honeycomb cell walls. It is only advised for thin panels with the skin face up. Hand sawing is for trimming on site. Ends: sealing as in section 9 is mandatory once cut. Leave 0.5 mm on the cut and finish to size, otherwise the edge is not straight. Holes: through holes must miss the core voids, or be pre-inserted. Above 20 mm diameter, add a reinforcing plate round the hole, or the skin bulges first at the edge.

Delivery states

  • 3K 2×2 twill Classic herringbone, the clearest pattern. The default for visible parts, stands and equipment enclosures.
  • 3K plain weave Checkerboard, finer than twill. For faces where the pattern has to be regular and panels pattern-matched.
  • 12K twill Larger check, coarser weave. For large panels: texture from a distance, less fine than 3K close up.
  • UD, unpatterned No weave, solid dark grey to black. Structural and internal parts, and faces to be primed for paint.
  • Forged carbon Irregular flakes, a forged look. Visible parts; no two sheets alike.
  • Natural The laminated skin as it comes, no coating; the cut edge sealed as part of the edge-sealing step. The default for structural and internal parts.
  • Clear coat (gloss or semi-matte) A coat over the weave. Gloss makes the pattern deeper and the colour darker; semi-matte sits between the two. Most visible parts take this.
  • Matte The same coating system, flattened; less reflection, fingerprints less obvious. Common on equipment enclosures and vehicle interiors.
  • Painted Painted to a project colour reference; colour and gloss are yours. Paint covers the weave — a pattern or paint, one or the other.

Tolerance and inspection

Overall thickness (≤20 mm) ±0.3 mm Micrometer + dimensional report
Overall thickness (>20 mm) ±0.5 mm Micrometer
Skin thickness ±10% (counted by plies) Calliper / ultrasonic
Edge ±0.5 mm Tape measure + dimensional report
Diagonal difference ≤1.5 mm Tape measure
Squareness 90° ±0.3° Engineer's square
Flatness 1.5 mm / m Surface plate + feeler gauge
Core position ≤2 mm Visual + calliper
Skin-to-core disbond Not permitted Tap test / ultrasonic C-scan (on request)
Hole and slot position ±0.01 mm CNC / CMM

Common questions

Sandwich panel or solid carbon sheet — which should I choose?

Whichever constraint is tighter, space or weight. With space to spare and weight to save, take the sandwich: at equal stiffness it is usually about a sixth of the solid weight. With space fixed and only a few millimetres to play with, take the solid sheet, because a sandwich needs thickness before the sandwich effect appears. Lots of holes, screws and point loads also favour the solid sheet — it is less work

Is thicker always better?

Thickness buys bending and adds almost no weight, so for a bending panel thicker is better value. But a thick panel costs twice over: it takes up height, and thin skins on a thick core dent more easily under local load. So when you add thickness, take the skin up with it; do not add core alone

Can I fix things to it and drive screws into it?

Yes, but prepare it first. Honeycomb cell walls are thin and a screw run straight in crushes them; foam cores will not take high torque either. Bury a solid block or potting compound at the fixing point, or use a through bolt with a large washer behind to spread the load. Mark every fixing point on the drawing and we handle it at layup

Will water get into a cut edge?

It will, and it is the commonest cause of failure in a sandwich panel. The cut edge has to be sealed: adhesive sealing indoors, a bonded-in frame or edge wrapping outdoors, in damp conditions or where the panel is washed. Sealing is decided at cutting; after the cut, adhesive sealing is all that is left

How is the areal weight calculated?

Two skins plus the core: 2 × skin × 1.55 + core × core density ÷ 1000, in kg/m². The table is already worked out, and adhesive film adds 0.1–0.3 kg/m². A solid carbon sheet of the same thickness is thickness × 1.55, for direct comparison

Why is there no strength or modulus in the table?

Flexural stiffness, flatwise compressive strength and shear strength all move with core type, core density, skin layup and adhesive film — writing a single figure down is a promise. Every geometric quantity is here: overall, skin, core, areal weight. Material data goes out with the quotation, for the combination you choose

What is the largest panel you can make?

Stock 1220×2440 mm, and 1000×2000. Larger depends on press size and core supply, quoted to drawing. Very large panels need transport thinking about — 2440 mm is already close to a standard lorry width

Can you drill, slot and counterbore it?

Yes, by CNC. Through holes must miss the core voids or be pre-inserted; above 20 mm diameter add a reinforcing plate, or the skin bulges at the edge. Hole position ±0.01 mm

Can the two skins be different thicknesses?

Yes. A bending panel has equal skins; where one face takes point load or carries fittings, thicken that face. Unequal skins move the neutral axis, so set it by the load direction and mark clearly on the drawing which face is up

What are the MOQ and lead time?

100 sheets. 20–25 days for stock combinations, including adhesive-film hot pressing; a non-standard overall thickness, a special core or a bonded-in frame takes 5–7 days

Can you use glass fibre skins?

Yes, in the same construction — lower cost, insulating, lower stiffness. Quoted through the glass fibre product line

Send us the size

Section, length, quantity and service conditions — with these in hand the quote is accurate. Upload a drawing if you have one; without one, the same figures written out will do.

No file selected

PDF, DWG, DXF, STEP, STL, ZIP or a phone photo — up to 20 MB.

The part, the material, the size — or the problem it has to solve. Drawings and photos can go in the field above.

+ Company, quantity, timeline

Used only to answer this enquiry and for related technical follow-up.

  • Company address Zhuyuan Tianhuan International, No. 76 Keji 2nd Road, High-tech Zone, Xi'an, Shaanxi, China
  • Factory Fengjing Industrial Park, Middle Section of Fengwu East Road, Huyi District, Xi'an, Shaanxi, China
  • Sales email sales@atomfrp.com
  • Phone (WeChat) +86 18191567691 Email and forms answered 24/7; phone Mon–Fri 09:00–18:00 GMT+8
  • WhatsApp +853 68617664 Email and forms answered 24/7; phone Mon–Fri 09:00–18:00 GMT+8
  • A named engineer replies within 24 hours
  • NDA can be signed before any file is sent
  • Drawings and requirements are not disclosed

Send the drawing. We will send the route.

A drawing, a photo of a failed part, or three lines of requirement is enough to start. Scope, price indication and lead time within 24 hours.

No commitment · NDA available · Reply within 24 hours

Request a quote WhatsApp