Reference image. The actual surface and colour depend on the resin and the finish.
Overview
Carbon fibre sheet (CFRP laminate). Full sheet 2440×1220 mm (4×8 ft), thickness 0.3–50 mm. Thickness tolerance ±0.1 mm, ±0.05 mm when ground; flatness 0.3 mm/m. 3K twill face, peel-ply back that bonds without sanding. Post-machining available: water-jet guided cutting, CNC milling, hole drilling, slotting, counterboring and chamfering; send a DXF layout and we nest the parts. Cut lengths come from here; a machined part comes from custom composite parts.
Read it by thickness. Sheet size is fixed and stated in the note; some thicknesses come in a reduced sheet, so do not mix the two in one request.
Code
Thickness
Stock sheet size
Process
Thickness tolerance
Flatness
Note
SH-0.3
0.3
2440×1220
Compression moulded
±0.05
0.3
Facing and shims
SH-0.5
0.5
2440×1220
Compression moulded
±0.05
0.3
Facing and thin panels
SH-0.8
0.8
2440×1220
Compression moulded
±0.05
0.3
Panels and covers
SH-1.0
1.0
2440×1220
Compression moulded
±0.05
0.3
Panels and covers
SH-1.2
1.2
2440×1220
Compression moulded
±0.1
0.3
Interior panel
SH-1.5
1.5
2440×1220
Compression moulded
±0.1
0.3
Light-duty structural sheet
SH-2.0
2.0
2440×1220
Compression moulded
±0.1
0.3
Robot mounting plate
SH-2.5
2.5
2440×1220
Compression moulded
±0.1
0.3
Gauge base plate
SH-3.0
3.0
2440×1220
Compression moulded
±0.1
0.3
Standard structural sheet
SH-4.0
4.0
2440×1220
Compression moulded
±0.1
0.3
Load-bearing plate and tooling
SH-5.0
5.0
2440×1220
Compression moulded
±0.1
0.3
Thickest full sheet
SH-6.0
6.0
1000×2000
Compression moulded
±0.1
0.3
Load-bearing plate
SH-8.0
8.0
1000×2000
Compression moulded
±0.2
0.3
Weight-saving, aluminium replacement
SH-10
10
1000×2000
Compression moulded
±0.2
0.3
Weight-saving, aluminium replacement
SH-12
12
1000×2000
Compression moulded
±0.2
0.3
Pressure block
SH-15
15
1000×2000
Compression moulded
±0.2
0.3
Mould base plate
SH-20
20
1000×2000
Compression moulded
±0.2
0.3
Pressure and mounting plate
SH-25
25
To drawing
Compression moulded
±0.2
0.3
Plate
SH-30
30
To drawing
Compression moulded
±0.2
0.3
Plate
SH-40
40
To drawing
Compression moulded
±0.2
0.3
To drawing
SH-50
50
To drawing
Compression moulded
±0.2
0.3
To drawing
The carbon fibre sheet range runs from 0.3 to 5 mm in full sheets of 2440×1220 mm; 6–20 mm shrinks to 1000×2000 mm, and thicker is to drawing. A 1 mm sheet is about 1.55 kg/m², so weight can be estimated from thickness. Thicknesses and sheetSizes outside the table are produced to drawing; MOQ is in the panel.
A rigid sheet is not a veneer People searching for "rigid carbon fibre sheet" are mostly avoiding one thing: the 0.5 mm self-adhesive veneer stuck onto plastic to pass as carbon fibre. There are no layers in its section, it bends at the first flex, and the edge is printed or a film. A real sheet is a laminate. Prepreg plies cured under pressure and temperature, with thickness set by the ply count. A section that shows ply after ply. You can tell on the spot, without instruments:
There is also a "flexible carbon fibre sheet" sold online, adhesive-backed, bends by hand. That is a decorative veneer rather than a laminate, and it is the thing we do not make. Otherwise we make laminates only, not veneers. Quotes are by thickness and sheet size rather than by the sheet. Cutting two parts or twenty out of one sheet costs the same in material.
Thickness from 0.3 to 50 mm, and each band does a different job
0.3–1.0 mm: panels, shims, models and light-duty covers. Thin sheet takes its thickness from the layup and does not suit long spans; the 0.3 mm band is essentially facing and shim work. 1.5–3.0 mm: standard structural sheet. Equipment panels, robot mounting plates, gauge base plates, the band that sells most, 4.0–6.0 mm: load-bearing parts and tooling. Where a thread is needed, use a bonded insert; do not tap straight into the plies. Above 5 mm the full sheet has to shrink. That is the industry rule, not our limitation. 8.0–15 mm: weight-saving parts that replace aluminium blocks. At this thickness flatness comes from the mould and from grinding afterwards, not from curing. 20–50 mm: plate, available with a forged finish. Moulds, pressure blocks, mounting plates that have to stay rigid. At this thickness we always recommend grinding both faces, otherwise the tolerance drifts through the middle of the sheet, thickness tolerance runs in bands. ±0.05 mm from 0.3 to 1 mm, ±0.1 mm from 1 to 6 mm, ±0.2 mm above 6 mm. Grinding brings any of them to ±0.05 mm. A thinner full sheet depends on whether the layup consolidates, confirm on the drawing at quotation.
Sheet size: a full sheet is 2440×1220, about 3 m²
A full sheet is made to 4×8 ft, that is 2440×1220 mm, about 3 m². Makers who press their own sheet run 1000×980 to 2000×1000, that is 1 to 2 m²; ours is one band up. The 4×8 format is sold as well, but it arrives as bought-in board cut down, not pressed in-house. What sheet size is worth is not "big", it is one joint fewer. A two-metre equipment panel needs two joints out of a 2 m² sheet, and every joint is a break in stiffness and in appearance. A full sheet has no such break. As thickness rises, sheet size has to give way. Above 5 mm the full sheet shrinks to 1000×2000, and thicker is to drawing, not because we cannot do it. Press tonnage and die rigidity decide, and suppliers everywhere work the same way. Give thickness and sheet size together when you order and we quote the largest workable size. Do not fix the size first and then ask whether it can be made that thick, a full sheet also saves material. Send a DXF layout and we place your parts on one sheet, with offcuts still yielding small parts. We quote the sheet price plus machining, usually less than buying by the part, the cost is transport. A full sheet ships in a wooden crate, freight by volume. Or we cut to your layout before dispatch, which brings the volume down and the freight with it. For anything larger, go to a sandwich. Two thin skins over a core, which gets the size up and the weight down, see carbon fibre sandwich panel.
Surface: one face, both faces, and layup
Gloss one face: natural finish with a clear coat, 3K twill on the face. Peel-ply texture on the back. That face is rough, and peeling the cloth away leaves a surface ready to bond without sanding, the commonest configuration for structural parts. Gloss both faces: both faces are visible faces. Used for dividers, exposed panels, and parts where both sides show once the assembly is opened. Costs more than one face, because it takes an extra surface operation. Matte: the same coating system, flattened; fewer fingerprints and reflections, common on equipment housings. Forged finish: chopped compound, compression moulded; the pattern has no direction, like marble. A cut edge exposes short fibre, so visible parts need an allowance and trimming afterwards. Surface is fixed at the layup and mould stage and post-machining cannot change it, so settle it when you order. Layup comes in quasi-isotropic and unidirectional (UD). Quasi-isotropic alternates 0°/90° with ±45°, so properties are close in every direction. The choice when the load path is not settled yet. Unidirectional puts all the fibre one way, stiffest in that direction, with 90° plies carrying the transverse load; drive parts and cantilevers use it. A UD sheet reads as an even matte black, which suits parts still to be painted. Our standard layup alternates 200 g/m² 3K twill with 300 g/m² ±45° biaxial, at 55–60% fibre by weight, about 1.55 kg/m² at 1 mm. If stiffness drives the design, give a target (N/mm. A natural frequency) and we build ply count and angles to it rather than guessing from thickness.
Delivery states
Gloss one face, peel-ply back 3K twill gloss on the face; the back bonds directly, without sanding (adhesive choice and bond strength per project).
Gloss both faces Both faces finished; for dividers and exposed panels.
Matte The same coating system, flattened; fewer fingerprints and reflections.
Forged finish Chopped moulding compound, pattern without direction; leave an allowance on cut edges and trim after.
Tolerance and inspection
Thickness (0.3–1 mm)
±0.05 mm
Micrometer + dimensional report
Thickness (1–6 mm)
±0.1 mm
Micrometer
Thickness (>6 mm)
±0.2 mm
Micrometer
Thickness (ground)
±0.05 mm
Micrometer
Flatness
0.3 mm/m
Surface plate + feeler gauge
Sheet size
±2 mm
Tape measure
Profile (cut parts)
±0.1 mm
Calliper
Hole position and slotting
±0.01 mm
CMM
Delamination and voids
Not permitted
Ultrasonic sampling
Common questions
Can you cut parts to drawing?
Yes. Water-jet guided cutting for the profile and holes, CNC milling for outlines, counterbores, steps and chamfers, with cut profile at ±0.1 mm and hole position at ±0.01 mm. Send DXF or STEP and we quote the sheet price plus machining, with parts cut to size. We do not cut threads into carbon fibre — fixing is by bonding, through bolts or bonded inserts
How do I tell your sheet is a real laminate and not a veneer?
The section shows layers, the back is peel-ply texture or carbon weave, and a 1 mm sheet is about 1.55 kg/m². A veneer shows a single film in section, has adhesive or plastic on the back, and is noticeably lighter
What thicknesses can you make?
0.3–50 mm. Thickness tolerance is ±0.05 mm up to 1 mm, ±0.1 mm from 1 to 6 mm, ±0.2 mm above 6 mm; grinding takes any of them to ±0.05 mm
What is the largest sheet you can make?
0.3–5 mm comes as a full sheet of 2440×1220 mm, 6–20 mm shrinks to 1000×2000 mm, and thicker is to drawing. A full sheet ships in a wooden crate, freight by volume; cutting to your layout before dispatch saves freight.
One face or both — which should I choose?
Structural parts take one face: the face is the visible one, and the peel-ply back bonds directly without sanding. Bond strength depends on the adhesive and on surface prep — test data ships with the sheet, and the adhesive is chosen alongside it. Gloss both faces is for parts seen from both sides, and costs a little more
Can you make a forged finish?
Yes, from chopped compound in a compression mould. The pattern has no direction, like marble; a cut edge exposes short fibre, so visible parts get an allowance and are trimmed afterwards.
Laser cutting or CNC milling — will the edge chip or burn?
Thin sheet and visible parts go to water-jet, which leaves a small heat-affected zone and does not burn the cut edge; thick sheet and irregular outlines go to CNC milling. Sawn edges need an allowance and trimming
Will the sheet warp?
The layup is symmetric, and flatness comes from the mould and from grinding afterwards rather than from cure, so what leaves the factory is 0.3 mm/m. The larger and thinner the sheet, the more temperature difference moves it; store and transport it flat, not standing against a wall
What are the MOQ and lead time?
200 full sheets for stock sizes; single sheets, a handful of panels or nested parts are taken on by arrangement, with no set-up charge. Normal batches ship in 15–20 days; non-standard thickness and sheet size are quoted separately
Can you make glass fibre?
Yes, in the same construction — lower stiffness and lower cost, common for insulating parts and low-frequency structural parts. Quoted through the glass fibre product line
Send us the size
Section, length, quantity and service conditions — with these in hand the quote is accurate. Upload a drawing if you have one; without one, the same figures written out will do.
Company addressZhuyuan Tianhuan International, No. 76 Keji 2nd Road, High-tech Zone, Xi'an, Shaanxi, China
FactoryFengjing Industrial Park, Middle Section of Fengwu East Road, Huyi District, Xi'an, Shaanxi, China