T profile or I beam — which should I choose?
Look at whether both faces need fittings. An I beam has a flange top and bottom, so it stands alone as a beam and fixes at both ends; a T has one flange, so it goes against an existing face, reinforces one side, and takes half the space. At the same size an I beam bends about 1.8 times better for 30% more weight, so the I is more efficient; the T's advantage is that it can be bonded on
Is a T profile the same as a T beam?
The section is the same — one flange, one web. The name is not. T profile and T section are how the trade describes the section, and competitors' pages use them; T beam is structural engineering usage, but its SERP mixes servo press line equipment, machine tool beams and steel T beams, so searching on it does not land on profiles. Search T profile and you land on profile makers
Why is the neutral axis not in the middle?
There is only one flange, so the material piles on one side. yc = (B·t + H² − t²) / (2(B + H − t)): the wider the flange and the thicker the wall, the closer the neutral axis comes to the flange. 100×50×5 puts it at 35% of the depth, 100×100×5 at 27%. Select on depth, not on flange width
Can it be fitted the other way up?
It can be fitted, but the load case has to be recomputed. The second moment of area is unchanged, while the compression side moves from the flange to the web tip. With one free edge the web is a cantilever plate, so the buckling stress is far below that of a flange supported on two edges, and the moment it can carry at the same Ix drops a long way. Where an inverted fit is unavoidable, give us span, load and support conditions and we work the buckling out for that orientation
Does a wider flange increase bending capacity?
Not at equal weight. 50×50×5 is 0.74 kg/m with Ix 11.3; double the flange width to 50×100×5 and it is 1.12 kg/m with Ix 13.6 — half as much weight again for 20% more second moment of area. Depth is what works: 100×50×5, at the same 1.12 kg/m, gives Ix 76.7
How do I bond a panel stiffener?
Bond the underside of the flange to the panel, bond line 0.2–0.5 mm, clamped cure. The flange face has to be abraded or blasted to remove release agent — ask for bonding-face preparation when ordering. Bolts at the ends locate the rib only; the bond line carries the load. Run both ends into a frame rather than stopping in mid-air
Is the flange face flat?
Held to 0.3 mm / 100 mm. On a bonded part this figure matters more than the outside dimensions: an uneven face gives an uneven bond line, and the joint starts to fail at the thinnest point. Ask for it separately on a stiffener job
Can you drill and tap it?
Drilling, notching and counterboring, all at ±0.01 mm. Carbon fibre is not threaded: for a bolted joint use through bolts with washers, or bond an insert in. When drilling a T profile, keep the holes clear of the radius where the web meets the flange
Is there any carbon weave?
No. Pultrusion gives a unidirectional finish — a layer of resin, dark grey to black. Carbon weave means overwrapping 3K prepreg, or changing to a moulded part
What are the MOQ and lead time?
300 pcs. Normal batches ship in 15–20 days; a non-standard depth, flange or wall, or an unequal section, needs a die, which takes 5–7 days
Can you make glass fibre?
Yes, in the same construction — lower stiffness and lower cost, common for insulating parts and low-frequency structural parts. Quoted through the glass fibre product line