Flat bar or square tube, which should I choose?
Look at whether the load runs in one direction. Bending in one direction, and fitting against a face, go to flat bar: less height, it can be bonded on, and holes are easy. Stiffness both ways, or torsion, goes to square tube: closed on four sides, an order of magnitude better in torsion. Many people fix two flat bars at right angles into a T to replace a square tube. The stiffness gets there, and two extra bonding operations with it
Can it replace a steel bar of the same size directly?
It will fit, and it will be softer. Carbon fibre has a lower modulus than steel, so deflection grows at the same size. Equal stiffness means a larger section, worked back from I_carbon = I_steel × 210 ÷ E_carbon. Weight is still on our side, but the advantage narrows from 80% to 60–70%. Steel also welds and taps, and a carbon bar does neither, so the joint detail has to be redone. Flat or on edge
How do I decide?
Bonded to a face as reinforcement: flat. Carrying bending on its own: on edge. On edge, watch lateral instability. The larger the unrestrained length over thickness, the worse it is; add a mid support, or change to square tube. The same 30×3 has I of 68 mm⁴ laid flat and 6,750 mm⁴ on edge, a hundred times apart. Fitted the wrong way round the bar does almost nothing
Will a 6000 mm bar be bowed?
It will have a natural bow. A property of pultrusion, worse the longer it is. We hold 1 mm/m, no more than 6 mm over the piece. Straighter means selecting stock, or tightening the die and the puller, and both change cost and lead time. Where the assembly is sensitive to straightness, cut shorter, or fit on edge with support
Can it be drilled, and can it be tapped?
Drilled, yes; tapped, no. Edge distance 2.5 × the hole diameter is the floor and a loaded joint wants 3–4 ×; a diamond drill, a sacrificial board behind. Load goes through friction from clamped bolts, not through bearing at the hole wall, carbon fibre has no yield point, the wall crushes first. For threads, bond in a metal insert, or use a through bolt with a backing plate
Can it be bent into a curve?
Yes, what bends is elastic, not set. Carbon fibre is elastic right up to failure, with no yield point: hold the radius above the minimum and it springs straight back. Go past it and the inner fibres crush and delaminate, a pale band showing before it breaks, how tight depends on thickness. The trade figure for epoxy pultrusion is a minimum bend radius of 100 × thickness. 0.5 mm takes a 50 mm radius and 5 mm needs 500 mm or more. In strain terms that is thickness ÷ (2 × radius) ≤ 0.5%, the same rule. 50×0.5 on a 50 mm radius lands exactly on it. Width does not enter the limit; it only sets how much force the bend takes and whether the bar twists on the way. Holding the curve is a job for the structure, bonded to a curved face, dropped into a groove, clamped under a plate. It springs back the moment the constraint comes off. A curve that arrives curved is made on a curved tool: radius pultrusion (the die travels the curve, from 40 mm radius. 300–500 mm common on thin sections), or press moulding, or winding
What is the minimum order?
500 pcs. Different lengths in the same size can go on one order, counted in total pieces. A non-standard width or thickness, holes, or end assembly are agreed per project
Can you cut to length?
Yes. 1000, 2000 and 3000 are the standard cuts and carry no extra charge; other lengths are charged per cut. A cut end is a sawn face; precision cutting to ±0.5 mm is charged separately
Can the surface be matte, or clear coated?
Yes. The default is the die face; for bonding take the grit face and save the abrading; exposed parts can take a clear coat. A flat bar is a unidirectional part with no weave, so there is no pattern option, pattern belongs to sheet and to profiles
Can you make it 100 mm wide?
No, width stops at 50 mm. Beyond that width it is a narrow sheet rather than a flat bar. At the same thickness it lies too floppy flat and too unstable on edge. Its real use overlaps sheet. Above 60 mm wide, look at carbon fibre sheet and have it cut into strips, that works out cheaper