Reference image. The actual surface and colour depend on the resin and the finish.
Overview
Pultruded carbon fibre angle, equal 10×10–100×100 mm, wall thickness 1–10 mm, cut to length. Continuous fibre runs through the die along the length, so tensile and bending performance along the length is best. Both legs are flat faces, which makes drilling, bolting and bonding straightforward. Leg tolerance ±0.2 mm (above 50 mm, ±0.3 mm), right angle 90° ±0.5°, inside radius set by the wall thickness. Weight per metre is in the table. 25×25×3 is 0.21 kg/m, 50×50×3 is 0.44 kg/m. The same sizes in steel angle are 1.12 and 2.31 kg/m. The same profile can be supplied as a machined part: custom composite parts.
Read it as leg × leg × wall. Equal and unequal legs are different products; for unequal, state which leg carries the load, because the open direction follows it.
Code
Legs
Wall
Length
Weight kg/m
Tolerance
Note
LA-10-1
10×10
1
1000
0.028
±0.2
Display stands and models
LA-12-1
12×12
1
1000
0.034
±0.2
Corner edging
LA-15-1.5
15×15
1.5
1000
0.063
±0.2
Corner edging
LA-20-1.5
20×20
1.5
1000
0.087
±0.2
Enclosure frame
LA-20-2
20×20
2
1000
0.11
±0.2
Enclosure frame
LA-25-2
25×25
2
1000
0.14
±0.2
Display stand and edge trim
LA-25-3
25×25
3
1000
0.21
±0.2
General reinforcing angle
LA-30-2
30×30
2
1000
0.17
±0.2
Panel corner
LA-30-3
30×30
3
1000
0.25
±0.2
Frame reinforcing angle
LA-35-3
35×35
3
1000
0.30
±0.2
Frame reinforcing angle
LA-40-3
40×40
3
1000
0.35
±0.2
Frame reinforcing angle
LA-40-4
40×40
4
1000
0.45
±0.2
Load-bearing angle
LA-50-2
50×50
2
1000
0.30
±0.2
Retaining edge and rail
LA-50-3
50×50
3
1000
0.44
±0.2
Retaining edge and rail
LA-50-4
50×50
4
1000
0.57
±0.2
Load-bearing angle
LA-50-5
50×50
5
1000
0.70
±0.2
Load-bearing angle
LA-60-4
60×60
4
1000
0.70
±0.3
Structural angle
LA-60-5
60×60
5
1000
0.86
±0.3
Structural angle
LA-70-5
70×70
5
1000
1.01
±0.3
Structural angle
LA-80-5
80×80
5
1000
1.17
±0.3
To drawing
LA-80-6
80×80
6
1000
1.38
±0.3
To drawing
LA-100-6
100×100
6
1000
1.76
±0.3
To drawing, new die
LA-100-8
100×100
8
1000
2.30
±0.3
To drawing, new die
The inside radius is set by the wall thickness. The table covers equal angle; unequal angle (such as 40×20×3) is made to drawing on a new die. Weight is calculated at 1.55 g/cm³, so the weight of an order, and its freight, can be estimated from length. 2000 mm and 6000 mm lengths are also supplied。Sizes outside the table are produced to drawing; MOQ 500 pcs.
The price of an open section: spring-back and twist
An angle is an open section. The two legs are never closed against each other, so it carries two built-in problems before you buy. Spring-back: after curing, the two legs open or close slightly and the right angle is not exactly 90°. We hold 90° ±0.5°, and at assembly the adhesive layer or a shim absorbs that. Do not expect it to close up like a machined part. Twist: a long length rotates slowly along its length, more so the thinner it is. We hold 1°/m, which means a 6000 mm length can be 6° out at the end. For long rails and long retaining edges, put the twist requirement on the drawing and we check it over your full length. Not scaled from 1 m. A closed section has neither problem, neither square tube nor round tube. For an edge frame that must not twist at all, mitre a square tube rather than forcing it out of angle.
How to read the size: leg × leg × wall
The trade writes 25×25×3. Both legs 25 mm, wall 3 mm. An equal angle has two legs of the same length; an unequal angle is written 40×20×3. The order of choosing is the reverse of what you might expect, wall first, then leg. Wall decides whether you can drill, and whether a tightened bolt will crush the leg; leg decides stiffness and contact area. Below 3 mm wall, an M6 bolt needs a washer; below 2 mm, bonding or riveting only. The inside radius is set by the wall thickness. The same rule as on the square tube and polygon pages: the fibre has to pass round the die corner. An inside radius smaller than the wall cannot be consolidated, leaving a resin-rich zone behind. A drawing calling for R below the wall thickness means compression moulding or machining.
How to fix it: a row of holes in each leg
Half the value of an angle section is in the shape. Half in the fact that each leg can be fixed separately. The usual routes:
Through bolts: a row of holes in each leg, through the parts being joined, washers and tighten. Hole position ±0.01 mm, and the hole diameter 0.2–0.5 mm clear of your bolt. Bonding: the whole leg goes down and the adhesive takes the shear. Abrade the surface or peel the cloth off first, and choose the adhesive by duty. Riveting: common on thin wall and on covers or liners that are not meant to come apart, a blind rivet is enough, no insert needed. Angle brackets and connectors we do not make, that is another trade. We make the profile, and machine the holes and ends to drawing.
Weight per metre: what you save against steel angle Carbon fibre at 1.55 and steel at 7.85 gives about an 80% reduction at equal volume. Every band in the table carries kg/m, for direct comparison with steel angle:
Note that this compares equal volume. Carbon fibre runs at about 70 GPa axially against about 210 GPa for steel. At the same size it is a third as stiff. Equal stiffness usually needs a larger section or a thicker wall, and the saving lands below 80%. For a real replacement, give us the load, the span and the allowed deflection: working back from stiffness beats estimating by volume.
Length, cutting and end facing
Standard lengths are 1000 mm and 2000 mm, with 6000 mm as the longest single length. 6000 mm is a truck and container length; anything longer needs a joint. Cut with a saw or by water-jet. Water-jet leaves a clean edge without chipping, so thin wall and visible parts take it. Thick wall and long runs take sawing, leaving 0.2 mm on the end to machine back, end squareness is held to ±0.5°. An angle end is two faces, one per leg, and both have to be square for a frame to close without a gap.
Delivery states
Natural The pultruded surface as it comes: smooth, dark grey to black, unpatterned. The default for structural and internal parts.
Clear coat A coat over the natural surface, gloss or semi-matte. More resistant to soiling.
Matte The same coating system, flattened; less reflection, common on exposed edge frames and display work.
Painted Painted to a project colour reference; the colour and the gloss are yours, and we control flatness and adhesion.
Tolerance and inspection
Leg (≤50 mm)
±0.2 mm
Calliper + dimensional report
Leg (>50 mm)
±0.3 mm
Calliper
Wall thickness
±5% (thin wall counted by plies)
Calliper / ultrasonic
Right angle
90° ±0.5°
Engineer's square + feeler gauge
Inside radius
Set by the wall thickness (equal to it)
Profile gauge / projector
Twist
≤1° / m
Surface plate measurement
Straightness
1 mm / m
Surface plate + feeler gauge
Length (cut to length)
±0.1 mm
Water-jet guided / CNC
End squareness
≤0.5°
Engineer's square
Hole position and slotting
±0.01 mm
CMM
Common questions
Can it replace steel angle, and how do I choose the size?
It can, but the order is reversed: steel angle is chosen by equal strength, carbon fibre has to be sized by stiffness. Carbon fibre has a lower modulus than steel, so at the same size the stiffness is lower and you usually go one band up in wall thickness or in leg. Give us load, span and allowed deflection, and we work the section back from stiffness — do not copy the old steel size across
What is the leg tolerance?
±0.2 mm up to 50 mm, ±0.3 mm above 50. An angle is an open section and sits one band looser than a square tube — after curing the legs open or close slightly, and stay that way. Tighter than that is quoted to drawing; it can be done, but it means selecting material
Will it twist?
It will, more so the thinner and longer it gets; we hold 1°/m. For long rails and long retaining edges, put the twist requirement on the drawing and we check it over the working length, not scaled from 1 m
Can you drill it, and what hole tolerance do you hold?
We can. Water-jet for the holes, CNC milling for counterbores and notches, hole position ±0.01 mm. Below 3 mm wall an M6 bolt needs a washer; below 2 mm we recommend bonding or riveting. We do not cut threads into carbon fibre: joints are bonded, through-bolted or riveted. or riveting only
Can the inside radius be smaller?
The inside radius is set by the wall thickness, and that is the process floor — the fibre has to pass round the die corner, and any smaller cannot be consolidated, leaving a resin-rich zone. A sharper corner means compression moulding or machining, at a different cost and lead time
Do you make equal and unequal angle?
Equal angle is stock, 10×10 to 100×100. Unequal angle (such as 40×20×3) is made to drawing on a new die, with MOQ agreed per project
Is there any carbon weave?
No. Pultrusion gives a unidirectional (UD) finish — a layer of resin, dark grey to black. Carbon weave means overwrapping 3K prepreg, or changing to a moulded part
What are the MOQ and lead time?
500 pcs. Normal batches ship in 15–20 days; a non-standard leg or wall needs a new die, which takes 5–7 days
Can you make glass fibre?
Yes, in the same construction — lower stiffness and lower cost, common for insulating parts and low-frequency structural parts. Quoted through the glass fibre product line
Do you make angle brackets and connectors?
No. Brackets, hinges and connection plates are hardware, a different trade. We make the profile, and machine holes and ends to drawing; where an assembly is needed, send the drawing and we quote per part
Send us the size
Section, length, quantity and service conditions — with these in hand the quote is accurate. Upload a drawing if you have one; without one, the same figures written out will do.
Company addressZhuyuan Tianhuan International, No. 76 Keji 2nd Road, High-tech Zone, Xi'an, Shaanxi, China
FactoryFengjing Industrial Park, Middle Section of Fengwu East Road, Huyi District, Xi'an, Shaanxi, China