Overview

Pultruded carbon fibre square tube, or carbon fibre square box section in British trade usage. Continuous carbon fibre is impregnated with resin and pulled through a die in one pass. The fibre runs the full length, so bending and axial stiffness are highest. The four flat faces take bolts, corner brackets and linear rails directly. Side 10×10–200×200 mm, wall thickness 1.0–10 mm, cut to length. Side tolerance ±0.1 mm (±0.2 mm above 50×50), squareness of adjacent faces ≤0.5°, cut to length within ±0.1 mm. Post-machining available: cutting, hole drilling, slotting, end facing, bonding and assembly. If the size you need is not in this table, it becomes a custom composite part.

Request a quote

Where it is used

  • Equipment frames and machine frames
  • Gantry beams and columns
  • Robot guarding and safety fencing
  • Inspection tooling and fixture frames
  • Conveyor and rail brackets
  • Display stands and structural support

Stock sizes in detail

Read it as side × wall. The corner radius follows the wall and is not a column; when the wall changes, check the inner side first.

Code Side Inner side Wall Length Tolerance Note
SQ-10-1.0 10 8 1.0 1000 ±0.1 Light-duty frame
SQ-12-1.0 12 10 1.0 1000 ±0.1 Bracket
SQ-14-1.0 14 12 1.0 1000 ±0.1 Bracket
SQ-15-1.0 15 13 1.0 1000 ±0.1 Frame
SQ-15-1.5 15 12 1.5 1000 ±0.1 Frame
SQ-16-1.0 16 14 1.0 1000 ±0.1 Equipment frame body
SQ-16-1.5 16 13 1.5 1000 ±0.1 Equipment frame body
SQ-18-1.0 18 16 1.0 1000 ±0.1 Equipment frame body
SQ-18-1.5 18 15 1.5 1000 ±0.1 Equipment frame body
SQ-20-1.0 20 18 1.0 1000 ±0.1 Frame
SQ-20-1.5 20 17 1.5 1000 ±0.1 Equipment frame
SQ-20-2.0 20 16 2.0 1000 ±0.1 Load-bearing frame
SQ-22-1.0 22 20 1.0 1000 ±0.1 Rail bracket
SQ-25-1.0 25 23 1.0 1000 ±0.1 Rail bracket
SQ-25-1.5 25 22 1.5 1000 ±0.1 Gantry beam
SQ-25-2.0 25 21 2.0 1000 ±0.1 Load-bearing frame
SQ-28-2.0 28 24 2.0 1000 ±0.1 Robot beam
SQ-30-2.0 30 26 2.0 1000 ±0.1 Machine frame column
SQ-30-2.5 30 25 2.5 1000 ±0.1 Machine frame column
SQ-35-2.5 35 30 2.5 1000 ±0.1 Machine frame beam
SQ-40-2.5 40 35 2.5 1000 ±0.1 Gantry frame
SQ-40-3.0 40 34 3.0 1000 ±0.1 Load-bearing column
SQ-50-2.5 50 45 2.5 1000 ±0.1 Beam
SQ-50-3.0 50 44 3.0 1000 ±0.1 Beam
SQ-50-5.0 50 40 5.0 1000 ±0.1 Heavy-duty machine frame
SQ-60-3.0 60 54 3.0 1000 ±0.1 Gantry
SQ-60-5.0 60 50 5.0 1000 ±0.1 Heavy-duty gantry
SQ-80-4.0 80 72 4.0 1000 ±0.2 Large machine frame
SQ-80-5.0 80 70 5.0 1000 ±0.2 Large machine frame
SQ-100-5.0 100 90 5.0 1000 ±0.2 Structural column
SQ-120-5.0 120 110 5.0 1000 ±0.2 To drawing
SQ-150-6.0 150 138 6.0 1000 ±0.2 To drawing
SQ-200-8.0 200 184 8.0 1000 ±0.2 To drawing

A square tube saves joints, not stiffness

The value of a square tube is in the flat faces. A part with four flat faces takes bolts, clamp plates, corner brackets, T-nuts and linear rails directly. No clamp collar or saddle to make up for a round tube. In structures such as equipment frames, gantry beams and fixtures. The number of joints often decides cost and assembly time more than the members themselves, the cost is in torsion. At the same weight, a closed square tube has less torsional stiffness than a round one. Parts whose main load is torsional should go back to round tube. A square tube trades a little torsional stiffness for easy assembly, and in frame structures that trade usually pays.

All the fibre is axial: good bending. Clamps must spread the load Pultrusion impregnates continuous fibre and pulls it through a die in one pass. All the fibre runs the length, so axial strength and bending stiffness are best, and the unit price sits below roll wrapping. The cost is that there is no hoop fibre through the thickness: the side walls have little crush resistance. Point clamping, a hard clamp in a vice or an over-torqued bolt will crush the side wall at the load point. A crushed wall does not come back. The answer is to spread the load, larger clamp plates and washers, an insert sleeve in the clamped length. Load points on corners that carry support, bonded inserts at bolt holes. For joints taken apart repeatedly, use a moulded part or metal-clad the clamped length.

Corner radius and wall thickness are fixed before the die is cut The four corners of a square tube are a fibre build-up zone. More resin, less fibre, and cracks start there. Outer corner radius is normally 2–4 mm. The inner corner radius is determined by the wall thickness, 1–1.5 mm. The fabric has to pass round the mandrel. An inside radius smaller than the wall thickness cannot be compacted, leaving resin-rich areas and voids. Measured on a stock 20×20×1.5 part: inner radius 1.4–1.5 mm, outer radius 3 mm. A sharp corner calling for R<1 mm cannot be pultruded; it goes to machining or compression moulding, at a different cost and lead time. Read wall thickness and corner radius together: thicken the wall without changing the radius and the resin-rich corner grows. Taking cure shrinkage and cracking risk with it. Section, R and wall thickness are fixed before the die is cut, and changing any one of them means a new die.

Twist and the cut end decide whether a frame sits flat A pultruded part comes out of the die with slight bow and twist. Held to 1 mm/m. On a 6000 mm length that is 6 mm at the far end, absorbed by joint clearance at assembly. Taken out by leaving stock and machining back. Parts are cut to length with a ±0.1 mm tolerance, and squareness of the cut end is held to ±0.5°. An end that is not square leaves a gap when two tubes butt together, and neither the bonded face nor the bolted face closes. 6000 mm is a truck length; anything longer is quoted as freight per part, and lengths are joined with bonded sleeves or corner brackets.

Surface: weave and UD

The outer fabric sets the pattern, 3K/12K twill is the most common. A woven finish, as European customers call it, plain weave is denser and flatter. UD uses unidirectional cloth and gives an even matte black, which suits parts still to be painted. The fabric is stretched slightly round the corners, so the pattern distorts there. That is a process feature, not a defect. If it matters, specify UD.

Delivery states

  • Natural with clear coat Gloss, weave clearly visible; the carbon weave shows as soon as the part is fitted — the default for most visible parts.
  • Matte The same coating system, flattened; fewer fingerprints and reflections, common on equipment housings and exposed structural parts.
  • Painted The surface can be painted to customer requirement; colour and final gloss are set per project.
  • Laser engraving Customer logo, part number or graphic engraved on the surface.

Tolerance and inspection

Side (≤50×50) ±0.1 mm Calliper + dimensional report
Side (>50×50) ±0.2 mm Calliper
Wall thickness ±5% (thin wall counted by plies) Calliper / ultrasonic
Inner corner radius Determined by the wall thickness (1–1.5 mm) Profile gauge / projector
Squareness of adjacent faces ≤0.5° Engineer's square + feeler gauge
Straightness and twist 1 mm / m Surface plate measurement
Length (cut to length, cut end square ±0.5°) ±0.1 mm Water-jet guided / CNC
Hole position and slotting ±0.01 mm CMM

Common questions

Can you cut, drill and slot to drawing?

Yes. Cutting to length, through holes, slotted holes, notches and end facing are all done in-house, with hole position and slotting at ±0.01 mm; holes can be machined coaxially from both faces in one set-up. Where a metal end fitting, corner bracket or flange is required, we supply the assembly. We do not cut threads into carbon fibre — connections are bonded, or use through bolts and bonded inserts.

Square tube or round tube — which should I choose?

Look at the joint. Flat faces take corner brackets, clamp plates, T-nuts and rails directly, so frames, beams and machine frames go square; parts in torsion, under internal pressure or telescoping go round. At the same weight a square tube has less torsional stiffness than a round one, and long-span drive parts have to allow for it. Mixing the two is normal: square for columns and beams, round for drive and telescoping

What connectors do you use on a square tube?

Pick by how often the joint comes apart. Permanent: bonding — abrade the end face or the side, then structural adhesive with a 0.2–0.5 mm bond line. Removable: through bolts with corner brackets — washers either side of the bolt hole spread the load, hole position ±0.01 mm, both faces machined coaxial in one set-up. High bending moment: bonded inserts — an aluminium or stainless insert bonded into the hole, so the load passes through the insert instead of pressing straight onto the carbon wall

What side tolerance and squareness can you hold?

Side length ±0.1 mm at 50×50 mm and below, ±0.2 mm above; squareness of adjacent faces ≤0.5°, straightness and twist 1 mm/m. Anything tighter goes to machined parts, quoted per part

How sharp can the corner be?

Outer corner radius 2–4 mm as standard; the inner corner radius is determined by the wall thickness (1–1.5 mm); both are set by the die. On the 20×20×1.5 stock size, inner radius 1.4–1.5 mm and outer radius 3 mm. An inner radius smaller than the wall thickness cannot be compacted, and leaves resin-rich areas and voids; R<1 mm cannot be pultruded at all, so it goes to machining or compression moulding. R is fixed at drawing stage and cannot be changed once the die is cut

Will clamping crush the side wall?

A point clamp will. A pultruded wall has no hoop fibre through the thickness, so a concentrated load crushes the side wall at the clamp point, and the crush does not come back. The answer is to spread the load: bigger clamp plates and washers, an insert sleeve in the clamped length, bonded inserts at bolt holes, load points on the corners. For assemblies taken apart repeatedly, add metal corner protection or switch to a moulded part

Can you make a telescoping joint?

Yes. A square inner tube runs inside a square outer one, and the four flat faces stop it rotating — it cannot slip round the way a round telescoping pair can. For hexagonal and octagonal sections see hexagonal carbon fibre tube. The outer tube is ground to ±0.05 mm, the inner tube matched to the clearance, 0.05–0.15 mm. For location, drill a row of holes in the inner tube for a spring pin, or add a guide slot. The pair comes from the same production batch, so batch-to-batch variation cannot leave them unable to fit

Can you make rectangular tube?

Yes. Rectangular tube runs on the same pultrusion process, with the section set by drawing and the wall quoted separately. A non-equal-sided section needs a new die, and MOQ is calculated by section perimeter

What are the MOQ and lead time?

500 pcs for stock sections; trial batches by negotiation. Normal batches ship in 15–20 days. A non-standard section needs a die, with tooling lead time and cost quoted by section

Send us the size

Section, length, quantity and service conditions — with these in hand the quote is accurate. Upload a drawing if you have one; without one, the same figures written out will do.

No file selected

PDF, DWG, DXF, STEP, STL, ZIP or a phone photo — up to 20 MB.

The part, the material, the size — or the problem it has to solve. Drawings and photos can go in the field above.

+ Company, quantity, timeline

Used only to answer this enquiry and for related technical follow-up.

  • Company address Zhuyuan Tianhuan International, No. 76 Keji 2nd Road, High-tech Zone, Xi'an, Shaanxi, China
  • Factory Fengjing Industrial Park, Middle Section of Fengwu East Road, Huyi District, Xi'an, Shaanxi, China
  • Sales email sales@atomfrp.com
  • Phone (WeChat) +86 18191567691 Email and forms answered 24/7; phone Mon–Fri 09:00–18:00 GMT+8
  • WhatsApp +853 68617664 Email and forms answered 24/7; phone Mon–Fri 09:00–18:00 GMT+8
  • A named engineer replies within 24 hours
  • NDA can be signed before any file is sent
  • Drawings and requirements are not disclosed

Send the drawing. We will send the route.

A drawing, a photo of a failed part, or three lines of requirement is enough to start. Scope, price indication and lead time within 24 hours.

No commitment · NDA available · Reply within 24 hours

Request a quote WhatsApp