Overview

Pultruded carbon fibre rod. Carbon fibre is impregnated with resin and pulled continuously through a die in one pass. All the fibre runs axially, so tensile and bending strength are highest. And, unlike a thin-wall tube, it has no wall to collapse under a point load. Diameter Ø0.25–100 mm, cut to length, and at the small end it also serves as a carbon fibre dowel in place of wood. Diameter tolerance is banded by diameter, ±0.05 mm when ground. Post-machining available: cutting, drilling, end facing, grinding and bonding. Weight per metre is in the table, so quotes and freight can be estimated from weight first. Where the catalogue stops and the drawing starts, see custom composite parts.

Request a quote

Where it is used

  • Robot links and pushrods
  • Drive shafts and small roller shafts
  • Equipment frames and support rods
  • Tent poles and kite rods
  • Tool handles and grips
  • Locating pins and fasteners

Stock sizes in detail

Read it by diameter. The weight column is the second thing to look at — double the diameter and the weight goes up four times, and freight follows it.

Code Diameter Tolerance Stock length Weight kg/m Note
RD-0.25 0.25 ±0.05 1000 0.00008 Probes and models
RD-0.5 0.5 ±0.05 1000 0.00030 Fine stiffeners
RD-1.0 1.0 ±0.05 1000 0.00122 Model frames
RD-1.5 1.5 ±0.05 1000 0.00274 Kite rod
RD-2.0 2.0 ±0.05 1000 0.00487 Tent pole
RD-2.5 2.5 ±0.05 1000 0.00761 Tent pole
RD-3.0 3.0 ±0.05 1000 0.0110 Model pushrod
RD-4.0 4.0 ±0.05 1000 0.0195 Kite rod and pushrod
RD-5.0 5.0 ±0.05 1000 0.0304 Small link
RD-6.0 6.0 ±0.05 1000 0.0438 Link and handle
RD-8.0 8.0 ±0.1 1000 0.0779 Link and support
RD-10 10 ±0.1 1000 0.122 Robot link
RD-12 12 ±0.1 1000 0.175 Pushrod and shaft
RD-14 14 ±0.1 1000 0.239 Tool handle
RD-15 15 ±0.1 1000 0.274 Tool handle
RD-16 16 ±0.1 1000 0.312 Drive shaft
RD-18 18 ±0.1 1000 0.394 Drive shaft
RD-20 20 ±0.1 1000 0.487 Drive shaft and roller shaft
RD-22 22 ±0.15 1000 0.589 Roller shaft
RD-25 25 ±0.15 1000 0.761 Support column
RD-28 28 ±0.15 1000 0.955 Support column
RD-30 30 ±0.15 1000 1.10 Load-bearing support
RD-35 35 ±0.15 1000 1.49 Load-bearing support
RD-40 40 ±0.15 1000 1.95 Aluminium rod replacement
RD-45 45 ±0.15 1000 2.47 Aluminium rod replacement
RD-50 50 ±0.15 1000 3.04 Steel rod replacement
RD-60 60 ±0.15 To drawing 4.38 To drawing, new die
RD-70 70 ±0.15 To drawing 5.97 To drawing, new die
RD-80 80 ±0.15 To drawing 7.79 To drawing, new die
RD-90 90 ±0.15 To drawing 9.86 To drawing, new die
RD-100 100 ±0.15 To drawing 12.2 To drawing, new die

A solid rod is not a thicker tube

A tube is hollow: its wall collapses under a point load and does not spring back. A solid rod has no such problem, which is why a solid carbon fibre rod takes local bearing, takes a drilled hole and works as a pin. A hollow carbon fibre rod — that is, a tube — dents at the clamp.

But do not expect solidity to make it stiffer. Bending stiffness goes with the fourth power of diameter, so at the same diameter, swapping a tube for a solid rod adds little stiffness and multiplies the weight several times over. The line is clear:

Bending and light: a large-diameter tube. Crush, shear, a drilled hole, a pin: a solid rod.

Said plainly, a customer will not price a solid rod against a tube. They are not two versions of one part.

Diameter from 0.25 to 100 mm

0.25–1 mm: model frames, probes, stiffeners, slender supports. In this band the battle is drawing evenly.

1–5 mm: tent poles, kite rods, model pushrods, small links. High volume, normal batches ship in 15–20 days.

6–20 mm: robot links, tool handles, fasteners, locating pins. The band where orders concentrate.

25–50 mm: drive shafts, roller shafts, support columns, load-bearing parts that replace aluminium rod.

60–100 mm: large supports and heavy-duty parts that replace steel rod. This band is made to drawing on a new die, quoted per piece, with lead time following the tooling.

Thin rod is hard on drawing evenly and on broken filaments; thick rod is hard on cure exotherm and core voids — different process problems, not one set of parameters scaled up. So thin and thick are not quoted in the same band, and that is not obstruction.

Straightness matters more than diameter tolerance

A diameter tolerance of ±0.05 mm a customer can confirm with a micrometer. A two-metre rod bowed by 3 mm is visible the moment it goes into the machine, and it will not go in.

Straightness in a pultruded rod comes from pulling tension and a balanced cure: it is held to 1 mm/m at the factory, and to no more than 6 mm over a 6000 mm length. For pushrods, links and antennas, tell us the working length and we check straightness over that length rather than scaling from 1 m — a 6000 mm rod can be true within a metre of each end and still bow in the middle.

For straighter than that, stock has to be selected or the die and puller tightened, at extra cost and lead time; ask at quotation.

A pultruded rod has no carbon weave

Out of the die it is resin over axial fibre: an even dark grey to black, with no weave. That is not a question of grade, it is the process — unidirectional (UD) fibre has no warp and weft, so it has no pattern.

For carbon weave: overwrap a layer of 3K prepreg and cure again (an extra operation, and the diameter grows slightly), or change to a roll-wrapped tube, which can be laid up in twill and plain weave. A rod cannot.

Saying this early saves the question after delivery: why is there no pattern?

By the metre or by the piece: work out the weight first

Every band in the table carries kg/m. A 20 mm rod is 0.49 kg/m, so 500 pieces at 1 m is 244 kg; a steel bar of the same size is 1.24 t. Swapping the same part to carbon fibre takes the weight to about a fifth — stiffness and strength are counted separately, and that does not fit in one sentence.

Freight and duty both follow weight, so settle the length before the quote:

Give one length and we quote both, for you to compare.

Delivery states

  • Natural The pultruded surface as it comes: smooth, dark grey to black, unpatterned. The default for structural and internal parts.
  • Clear coat A coat over the natural surface, gloss or semi-matte. More resistant to soiling, and fewer fingerprints left at assembly.
  • Matte The same coating system, flattened; less reflection, common on exposed support rods and handles.
  • Painted Painted to a project colour reference; the colour and the gloss are yours, and we control flatness and adhesion.

Tolerance and inspection

Diameter (≤6 mm) ±0.05 mm Micrometer + dimensional report
Diameter (over 6 to 20 mm) ±0.1 mm Micrometer
Diameter (>20 mm) ±0.15 mm Micrometer
Diameter (ground) ±0.05 mm Micrometer
Ovality ≤0.05 mm Micrometer, several points
Straightness 1 mm/m; ≤6 mm over a 6000 mm length Surface plate + feeler gauge
Length (cut to length) ±0.1 mm Water-jet guided / CNC
End squareness ≤0.5° Engineer's square
Delamination and dry fibre Not permitted Visual + ultrasonic sampling

Common questions

Solid rod or tube, which should I choose?

Bending and light go to the tube: stiffness comes from the outside diameter. The bigger the diameter the stiffer it is, with a hollow middle and less than half the weight. Crush, shear, a drilled hole and pins go to the solid rod, which has no wall to collapse; a hollow rod is a tube. They are not two versions of one part, so do not price them by weight

Is the "graphite rod" sold online the same thing?

In fishing and model circles, graphite is an old name for carbon fibre and means the same material. In industry, though, a graphite rod, or a carbon electrode, is usually graphite: welding, arc and electrolysis duty. That is graphite, not carbon fibre, and it is an order of magnitude weaker. Look at the section before buying: a carbon fibre rod shows fibre, an electrode is uniform black grain

How thin and how thick can you go?

Ø0.25–100 mm. The 0.25 mm band is pulled from fine tow, mainly for probes and model parts. Ø60 and above is made to drawing on a new die, with lead time following the tooling

What diameter tolerance do you hold?

±0.05 mm to 6 mm, ±0.1 mm from 6 to 20 mm, ±0.15 mm above 20 mm. ±0.05 mm across the board after grinding. These are the shelf bands the trade quotes, and we quote the same set, why does MOQ band by diameter. Because the weight climbs fast. 500 pieces of Ø10 at 1 m is 61 kg; 500 of Ø100 at 1 m is 6 tonnes. Thick rod is quoted per piece so that a first order does not tie up tonnes of material, can you cut parts to drawing. Yes. Post-machining is all done in-house. Water-jet guided cutting, CNC milling, drilling, end facing and grinding, with cut length at ±0.1 mm and hole position at ±0.01 mm. We do not cut threads into carbon fibre; connections are bonded, through-bolted, insert-bonded or clamped

Is there any carbon weave on the surface?

No, pultrusion gives a unidirectional finish. A layer of resin, dark grey to black. Carbon weave means overwrapping 3K prepreg, or changing to a roll-wrapped tube

Will clamping crack it?

It will. The failure mode of a pultruded rod is longitudinal splitting: the teeth of a hard jaw, a clamp collar with too much interference. An over-tightened pipe clip, any of them bites into the surface and then splits along the fibre. Soft jaws on the clamped length, a rubber pad, or spreading the clamping force over a longer section, and there is no problem

Can you make glass fibre?

Yes, in the same construction, lower stiffness and lower cost, common for insulating parts and low-frequency structural parts. Quoted through the glass fibre product line

How much lighter is it than a steel rod?

At equal volume, carbon fibre at 1.55 and steel at 7.85 gives about an 80% reduction. But equal stiffness is not equal volume, steel has the higher modulus, so it has to be worked out from your load and span. Give us the duty and we can quote a replacement. Mechanical data, tensile, compressive, flexural and interlaminar shear, is supplied per project, so design to measured values rather than a brochure typical

Send us the size

Section, length, quantity and service conditions — with these in hand the quote is accurate. Upload a drawing if you have one; without one, the same figures written out will do.

No file selected

PDF, DWG, DXF, STEP, STL, ZIP or a phone photo — up to 20 MB.

The part, the material, the size — or the problem it has to solve. Drawings and photos can go in the field above.

+ Company, quantity, timeline

Used only to answer this enquiry and for related technical follow-up.

  • Company address Zhuyuan Tianhuan International, No. 76 Keji 2nd Road, High-tech Zone, Xi'an, Shaanxi, China
  • Factory Fengjing Industrial Park, Middle Section of Fengwu East Road, Huyi District, Xi'an, Shaanxi, China
  • Sales email sales@atomfrp.com
  • Phone (WeChat) +86 18191567691 Email and forms answered 24/7; phone Mon–Fri 09:00–18:00 GMT+8
  • WhatsApp +853 68617664 Email and forms answered 24/7; phone Mon–Fri 09:00–18:00 GMT+8
  • A named engineer replies within 24 hours
  • NDA can be signed before any file is sent
  • Drawings and requirements are not disclosed

Send the drawing. We will send the route.

A drawing, a photo of a failed part, or three lines of requirement is enough to start. Scope, price indication and lead time within 24 hours.

No commitment · NDA available · Reply within 24 hours

Request a quote WhatsApp