Overview

Tapered carbon fibre tube. The outside diameter changes continuously along the length, large end and small end set by drawing. With a continuous cone between them and no step. Roll wrapped, filament wound or compression moulded, with fibre laid along the generator. The wall can be uniform along the length or thickened in sections. It also appears as tapered carbon tube or conical, the same part either way. Against a constant-diameter tube, a tapered one puts material where the bending moment is. Thickest at the root of a cantilever, thinnest at the tip. Weight comes out while deflection stays inside limits. That is why rods, telescopic joints and diagonal braces use it instead of straight tube. If the size you need is not in this table, it becomes a custom composite part.

Request a quote

Environment and properties

Salt spray, chemicals, magnetic fields and temperature swings all answer differently in carbon fibre than in metal, so read this before choosing the material.

No rust, and it holds up against most chemicals: carbon fibre does not react with water or oxygen, so corrosion does not arise. On a coast, on a boat, at a pool, in a plating shop or on a wash line, a metal part shows rust within months while the carbon part is still die-face; and a scratch does not spread under a coating the way it does on a plated part. At room temperature it resists most acid, alkali and salt solutions, oils, alcohols and most solvents, and is stable against dilute acid, brine, fuel and hydraulic oil. What it does not resist has to be said as clearly: strong alkalis, strongly oxidising acids and strong solvents such as acetone attack or swell the resin, so check the medium, its concentration and its temperature at the material-selection stage. Above room temperature the resin sets the limit — a standard epoxy runs continuously to 80 °C and a higher-temperature system goes further, so fix the medium temperature first and then the resin.

Outdoors it needs UV protection: epoxy is affected by ultraviolet, and long exposure powders the surface and exposes fibre. A clear coat or a polyurethane topcoat holds it off and the substrate is unaffected. It will survive uncoated too, it just goes progressively duller.

In contact with metal it needs isolation: carbon fibre conducts, and against aluminium, steel or zinc with an electrolyte present — rain, condensate, salt spray — it forms a galvanic couple in which carbon is the cathode and the aluminium goes first. Put a glass-fibre washer or an insulating coating in the interface and insulate the bolts, and in a marine environment this is not optional.

Non-magnetic and low expansion: neither carbon fibre nor epoxy is magnetic, so next to MRI equipment, electron microscopes and precision sensing it introduces no disturbance — but it does conduct, so electrical isolation means a glass-fibre part. The axial coefficient of thermal expansion is close to zero: over 40 °C, a two-metre steel part grows 0.9 mm and a carbon one hardly moves, and that is what measuring machines, optical tables and antenna mounts are buying. Hoop expansion is larger than axial, so a mating part has to be calculated in both directions separately.

Light, but not equal stiffness at equal volume: density 1.55 g/cm³, a fifth of steel and three fifths of aluminium at equal volume. Equal volume is not equal stiffness — carbon fibre has a lower modulus than steel, so equal stiffness means working back through the section, and even then the weight figure has to include the fixings and any ballast.

Where it is used

  • Robot arms and links: stiffness at the root, less weight at the tip, the taper following the bending moment; Drive shafts and roller shafts: long span, no sag in the middle, a taper saves weight against constant diameter; Posts and bracing: masts and tie rods, thick at the root and thin at the tip; Tooling and mandrels: a taper locates, loads and unloads quickly, repeatability comes from the fit on the cone; Telescopic structures: telescopic joints with cone-to-cone engagement; Rods: tent poles and flagpoles, kite rods and fishing rod blanks

Stock sizes in detail

Read it as large OD → small OD plus length. The taper is derived, not tabulated; second moment is given at both ends and interpolates on the fourth power of the diameter in between.

Code Large end OD Small end OD Taper Wall I large end mm⁴ I small end mm⁴ Length Note
TT-12-08 12 8 1:125 0.75 421 113 500 Tie rod, bracing
TT-16-10 16 10 1:120 1.0 1,331 290 720 Post
TT-20-12 20 12 1:100 1.0 2,701 527 800 Telescopic outer tube
TT-25-15 25 15 1:100 1.5 7,676 1,467 1000 Support rod
TT-30-18 30 18 1:83 1.5 13,674 2,668 1000 Mast
TT-35-20 35 20 1:67 2.0 28,329 4,637 1000 Structural rod
TT-40-25 40 25 1:67 2.0 43,216 9,628 1000 Load-bearing rod
TT-50-30 50 30 1:50 2.5 105,507 20,586 1000 Large support
TT-60-35 60 35 1:40 3.0 218,780 38,943 1000 Load-bearing main rod
TT-80-45 80 45 1:29 3.0 538,657 87,728 1000 Large diameter
TT-100-60 100 60 1:25 4.0 1,392,153 277,264 1000 Large diameter
TT-150-90 150 90 1:17 5.0 5,993,079 1,210,004 1000 To drawing

Forming: roll wrapping, filament winding, compression moulding

All of these give a cone, the difference is what length, wall and ends they can produce. Roll wrapping: prepreg is wrapped ply by ply on a tapered mandrel, cured and demoulded. Thin wall, long parts and any taper are possible, and the length is set by the mandrel. A wall of 0.5–5 mm is the usual band, and tapers as gentle as 1:300 are made for rod work. Most tapered tube on the market is made this way. Filament winding: fibre is laid on the tapered mandrel at an angle, with hoop and longitudinal plies controlled separately. Suits diameters above 80 mm, and parts that must resist torsion or internal pressure. Winding a cone needs four-axis equipment or more, with the program corrected along the length as the diameter changes. Compression moulding: two steel mould halves close, press and heat, with prepreg or chopped compound placed in the cavity. Suits short cones, thick walls, and parts with a flange or stiffener at the end moulded as one piece, length usually up to 500 mm. Tapers as steep as 1:10. The advantages are an end form moulded in one shot, local thickening of the wall, and the lowest unit price at volume. The cost is the steel tool, and changing a dimension means changing the tool. Choosing: long, thin-walled or gentle taper goes to roll wrapping. Large diameter and hoop strength go to winding. Short, thick, complex-ended and in volume goes to moulding. Where more than one process can do the size, put the tooling cost into the comparison.

Large end, small end, length: the taper is calculated

The trade writes 30 → 18 × 1000. 30 at the large end, 18 at the small end, 1000 long, in mm. The taper is calculated from the end diameters and the length and is not listed separately, nor should it be. The same 1:83 can run 30 to 18 over 1000, or 60 to 36 over 2000, and those are not the same part. Taper is the ratio of the diameter difference to the length rather than an angle. 1:83 means the diameter falls by 1 mm for every 83 mm travelled. Some drawings give a half-angle instead, which has to be converted and is easy to get wrong. Put the diameters and the length on the drawing and there is nothing to misread. Large end and small end the other way round makes no difference to the process, only the ply order is reversed. Mark on the drawing which end is the datum, or the part will not line up at assembly, length is the hard constraint. With one mandrel, fixing the length fixes both end diameters. Changing the length means changing the taper or the end diameters. So give large end, small end and length together, with one missing, the order stops.

Change the taper and the layup changes with it

Prepreg for a straight tube is a constant-width strip, wrapped straight on. A tapered tube's circumference changes along its length. The material has to be cut as a sector. That is the fundamental difference between tapered and straight roll wrapping. The reason a tapered tube costs more. Roll wrapping: prepreg is cut to the developed pattern as sectors and wrapped ply by ply on the tapered mandrel. The steeper the taper, the greater the difference in arc between the two edges of the sector. The more material is wasted in the cut. Filament winding: fibre follows a geodesic path. On a cone the geodesic is not a constant pitch. The same winding angle at the large end corresponds to a different local angle at the small end. The program is corrected along the length as the diameter changes. The steeper the taper, the more the angle drifts, and beyond a point the fibre piles up or spans the surface. Why a straight-tube layup cannot be copied: a straight tube in 0/±45/90 carries the same stress distribution at every point along its length. A tapered tube's bending moment changes along the length, and the same ply works several times harder at the root than at the tip. Copy the straight-tube layup across and the usual result is an over-thick small end and an under-built root. Where a steep taper stops: past 1:10 the fibre starts sliding on the mandrel and resin-starved patches and wrinkles appear. The part is made in two sections and butt-joined. The joint position is set on the drawing. It is made as a joined part, not as one length.

How wall thickness is distributed along the length <strong>Uniform wall</strong> is the usual answer: the sector cut is compensated for the change in circumference. The wall comes out the same along the length. Weight is predictable and the internal cone is easy to machine. The downside is that the radius-to-thickness ratio is high at the small end, and that is where local crush resistance is weakest. <strong>Variable wall</strong> is built by section: a ply added at the small end, or a transition band in the middle. It suits a small end that has to take pressure, be drilled or carry a fitting. The transition leaves a step and the bore needs grinding, so it costs more than uniform wall. <strong>The small end is the weak point</strong>. This is where a tapered tube differs from a straight one: a straight tube has the same section throughout. The small end of a tapered tube has the smallest diameter at the same wall. Its bending section modulus is the lowest and it buckles locally first under compression. Design it as if it were an equal-strength section and it will usually come up short.

A tapered beam does not follow the constant-section formula

The second moment of area of a tapered tube changes along the length. Following the fourth power of the diameter as I(x) = π(D(x)⁴ − d(x)⁴) ÷ 64. A cantilever in tapered tube deflects more at the tip than a constant-diameter tube of the same length and root section. The textbook pL³/3EI under-reads it. The same fact is why a taper pays. A cantilever's bending moment falls linearly from root to tip. Making the diameter fall linearly as well puts the material where the moment is, and weight comes out without adding deflection. In an equal-strength design, the peak bending stress at the root and at the small end come out close to equal. To work out the deflection, large-end OD, small-end OD and wall are enough, with span and tip load. We integrate in steps along the length rather than quote a single stiffness. A single EI for a tapered tube means nothing.

Straightness, concentricity and ends

Straightness: held to 1 mm/m, and no more than 6 mm over the piece. A tapered tube is harder to hold than a straight one, because the wall changes along the length and uneven cure shrinkage amplifies bow. Concentricity: the offset of the two end centres from the axis, normally 0.2 mm. It matters most on telescopic fits and on assemblies, on a cone-to-cone fit a concentricity error turns straight into run-out, run-out at speed is vibration. Ends: after cutting, the end face is perpendicular to the axis, normally 0.2 mm. Where the end face has to bear load, butting against a fitting, say. It goes on a milling machine rather than just a saw. Grinding: the outside can be ground to ±0.05 mm at Ra 1.6. Grinding a cone needs a dedicated fixture, so it is quoted per piece.

Jointing: taper fits, bonding, drilling

A taper fit is the natural joint: an inner cone in an outer one. Torque and centring carried by the contact, no key needed. The requirements are matched tapers and enough contact. A blue check should show 80% or better. Below that the torque capacity falls away faster than expected. A gentle taper self-locks: the gentler the taper, the smaller the half-angle, and the harder it is to pull apart once seated. Tapers of 1:20 and gentler essentially self-lock, so leave jacking-thread holes for disassembly or make a two-part clamp collar. For repeated tool-free assembly the answer is not the taper at all, it is a clamp collar or a locking ring. Bonding: structural adhesive on the cone, assembled and cured. Load goes through shear in the bond line over a large area, which makes it the most reliable way to fix a tapered tube. The one you cannot take apart. Drilling: drill normal to the cone surface, never parallel to the axis. An angled hole through a thin cone splits it. Edge distance starts at 2.5 × the hole diameter, and 3–4 × on a loaded joint, No tapping. The wall on a cone is limited and a thread cut straight into it will not hold. For a thread, bond a metal insert into the end, or use a through bolt with a backing plate. Reinforce the ends: where a fitting puts concentrated load on the end, add plies or an insert sleeve, the cone crushes under bolt preload.

Delivery states

  • Natural (die face) The surface straight off the mandrel or mould — smooth, and can be bonded as it is (a grit finish is safer)
  • Grit face Abraded, saving a step before bonding
  • Clear coat A coat on the die face, deeper colour, better weathering
  • Ground Outside ground to ±0.05 mm, for fits and sliding faces
  • Machined Ends milled flat, holes drilled, slots cut, to drawing

Tolerance and inspection

Large-end OD ±0.1 mm (ground ±0.05) Calliper / micrometer
Small-end OD ±0.1 mm (ground ±0.05) Calliper / micrometer
Wall thickness ±0.1 mm Micrometer
Taper ±0.05 mm / 100 mm (ground ±0.03) Back-calculated from both ODs and length
Length ±0.5 mm Tape
Straightness 1 mm/m, no more than 6 mm over the piece Surface plate and feeler gauge
Concentricity 0.2 mm (ground 0.1) Dial indicator
End squareness 0.2 mm (ground 0.1) Square

Common questions

How steep a taper can you make?

The gentle end runs to 1:300, which is where slender rod work sits; structural parts and joints usually sit between 1:50 and 1:15. Steeper than 1:10 the fibre begins to slide on the mandrel and wrinkles and resin-starved patches appear. Roll wrapping and winding switch to two sections butt-joined. For a one-piece part, go to compression moulding

Can the small end be closed?

Yes, with an end cap or a closed end. A closed end is simplest in compression moulding. Closing a roll-wrapped or wound part needs a dedicated mandrel, and the wall of the dome and the transition have to be designed together. A step change collects resin

Can the wall be thick at one end and thin at the other?

Yes. Roll wrapping adds plies by section, which leaves a step at the transition and needs the bore ground. Compression moulding does it in the cavity with no step. Put the added plies where your bending moment diagram says, not at the thinnest point of the small end

Can you make a telescopic joint?

Yes. The two tapers have to match, and the fit centres on the cone. The critical points are taper and concentricity: a gentle taper self-locks and needs something to push it apart. Concentricity has to be held to 0.1 mm or the extended part runs out. The pair comes from the same production batch; do not order them in separate batches

Will it survive at the coast or in chemical service?

Yes. It does not rust and resists most acids, alkalis, salts and solvents at room temperature. Keep it away from strong alkalis, strongly oxidising acids and strong solvents. Add a clear coat outdoors against UV. And isolate it wherever it meets aluminium or stainless steel

Is it magnetic, and will it disturb sensors?

No. Neither carbon fibre nor epoxy is magnetic, so it introduces no disturbance near MRI, electron-beam or precision sensing equipment. It does conduct, though, so electrical isolation means a glass-fibre version or an insulating pad, does the length change with temperature. Hardly at all axially. The expansion coefficient is close to zero, more than an order of magnitude below steel. Hoop expansion is larger, so mating parts are calculated on the hoop direction

Can a tapered tube be bent into an arc?

It can be bent, but only elastically and at a large radius. For a tube of outside diameter D and bend radius R the outer fibre strain is D ÷ (2R), keep it under 0.5%. A 30 mm tube needs a 3 m radius. Bending also takes the roundness out of the section, and a cone fit no longer works after it. For a curved tapered tube, the part is made on a curved mandrel; it is not a straight cone bent afterwards

Can it be drilled, and can it be tapped?

Drilled, yes; tapped, no. Drill normal to the cone surface and keep edge distance from 2.5 × the hole diameter. On a loaded joint use a metal insert or a through bolt

What is the MOQ?

Agreed per project. Small batches of stock sizes are accepted. A non-standard taper needs a tapered mandrel, so the MOQ follows the tooling amortisation. A moulded part needs a steel tool, and the MOQ follows that

What does a taper buy over straight tube?

Material that follows the bending moment: thick at the root, thin at the tip, lighter for the same deflection limit. And a larger diameter at the joint, which gives more bond area and better crush resistance than straight tube of the same weight. The price is a higher unit cost, a longer lead time, and a layup to recalculate every time one number changes

Can the surface be matte, or clear coated?

Yes. The default is the die face; for bonding take the grit face and save the abrading; exposed parts can take a clear coat. A tapered part has no weave option. That belongs to sheet and to moulded parts, since roll wrapping and winding give a unidirectional or twill face

Send us the size

Section, length, quantity and service conditions — with these in hand the quote is accurate. Upload a drawing if you have one; without one, the same figures written out will do.

No file selected

PDF, DWG, DXF, STEP, STL, ZIP or a phone photo — up to 20 MB.

The part, the material, the size — or the problem it has to solve. Drawings and photos can go in the field above.

+ Company, quantity, timeline

Used only to answer this enquiry and for related technical follow-up.

  • Company address Zhuyuan Tianhuan International, No. 76 Keji 2nd Road, High-tech Zone, Xi'an, Shaanxi, China
  • Factory Fengjing Industrial Park, Middle Section of Fengwu East Road, Huyi District, Xi'an, Shaanxi, China
  • Sales email sales@atomfrp.com
  • Phone (WeChat) +86 18191567691 Email and forms answered 24/7; phone Mon–Fri 09:00–18:00 GMT+8
  • WhatsApp +853 68617664 Email and forms answered 24/7; phone Mon–Fri 09:00–18:00 GMT+8
  • A named engineer replies within 24 hours
  • NDA can be signed before any file is sent
  • Drawings and requirements are not disclosed

Send the drawing. We will send the route.

A drawing, a photo of a failed part, or three lines of requirement is enough to start. Scope, price indication and lead time within 24 hours.

No commitment · NDA available · Reply within 24 hours

Request a quote WhatsApp