L profile or box section — which should I choose?
Load at the edge and a corner to sit into: the angle. Closed on four sides and torsion to resist: box section. For light guardrail and walkway edge strip, an angle uses less material.
Reference image. The actual surface and colour depend on the resin and the finish.
It does what steel angle does, without the rust. Frames, corner capping, angle bracing, stair nosing, cable tray brackets, wherever galvanised steel angle was used and the medium is acidic or alkaline. The part must not conduct, this replaces it. Density 2.0, a quarter of the weight of steel at the same section. A 6 m length of 50 × 50 comes in at a little over five kilos: one person carries it. The two legs meet at a right angle. Putting the profile against a corner gives you a 90° datum without a separate setting-out block. On a box corner the two legs land on two faces at once, with a row of bolts down each leg. The joint has one gap fewer and one alignment fewer than two flat plates mitred together. Equal leg from 25 to 150 mm, wall 3 to 12 mm, commonly in 6 m lengths. Equal angle covers general frames and bracing, unequal legs are made to drawing. The narrow leg against a panel, the wide leg carrying load, which saves both material and space. Load is carried by the section of the two legs rather than by piling on wall thickness. The centroid of an L sits out at the corner. The two directions do not have the same second moment of area: the load has to line up with the leg orientation. The same profile laid on its side carries much less. Draw the load direction on the selection sheet; it is more use than the leg length alone. Glass fibre is abrasive, so cutting, drilling and milling are all done in house. The water-jet guided laser also cuts to length and drills holes. It wears tooling faster than carbon fibre, and the extra tool consumption and slower cycle show up in the machining charge. A cut end exposes fibre, so parts for outdoor or damp service are sealed before dispatch. For a finished part rather than a length of stock, the route is custom composite parts.
kg/m is section area × density at 2.0 g/cm³; the section area is given alongside so you can check it.
| Leg mm | Wall mm | Section mm² | kg/m | Typical use |
|---|---|---|---|---|
| 25 × 25 | 3 | 141 | 0.28 | Light frame, cover |
| 30 × 30 | 3 | 171 | 0.34 | Decorative frame, support |
| 38 × 38 | 4 | 288 | 0.58 | Frame, bracket |
| 40 × 40 | 4 | 304 | 0.61 | Edge frame, post |
| 50 × 50 | 3 | 291 | 0.58 | Edge support, railing |
| 50 × 50 | 5 | 475 | 0.95 | Load-bearing edge frame |
| 50 × 50 | 6 | 564 | 1.13 | Load-bearing bracket |
| 51 × 51 | 6.35 | 607 | 1.21 | Joint facing piece |
| 60 × 60 | 6 | 684 | 1.37 | Platform edge beam |
| 60 × 60 | 8 | 896 | 1.79 | Main edge beam |
| 75 × 75 | 6 | 864 | 1.73 | Long-span edge frame |
| 75 × 75 | 10 | 1400 | 2.80 | Load-bearing edge beam |
| 100 × 100 | 8 | 1536 | 3.07 | Main structural bracing |
| 100 × 100 | 10 | 1900 | 3.80 | Heavy-duty bracing |
| 150 × 150 | 12 | 3456 | 6.91 | Heavy-duty post |
| 100 × 50 (unequal) | 8 | 1136 | 2.27 | Single-side load-bearing edge frame |
kg/m is section area × density at 2.0 g/cm³: for an equal angle, A = t(2a − t); for an unequal angle, A = t(a + b − t). The figure excludes the surface veil and the resin-rich layer, so actual weight runs 3–5% above the table; add 5% when quoting freight. Leg sizes, walls and unequal combinations outside the table are scheduled to drawing.
Edge trim. Corner capping and bracing is where an L profile belongs in a structure. Trim wraps a panel edge, hiding the cut and adding stiffness. Corner capping takes the corners of a box or a cabinet. Bracing does the diagonals and the stiffening, against box section. A box tube is closed on four sides and resists torsion. It will not sit into a corner. It needs a connection plate made up for it. An angle opens to take exactly one right angle, and one part does the corner, against flat bar. Flat bar covers one face only, so a corner needs two pieces and two fixings. One angle does the job of both, and locates itself. For light guardrail, machine guarding and walkway edge strip, an angle uses less material than box section. The load is at the edge anyway. The middle of a box is doing nothing.
Equal legs are symmetric, so the joint is symmetric and the part cannot go on the wrong way round. One stock item covers the job. General frames, bracing and corner capping all use it, unequal legs divide the work. The narrow leg bears on a panel as edge trim while the wide leg carries load, or the other way round. Wide leg as a foot, narrow leg as a stop. Grating edge support, panel closing and cable tray side fixing all go this way. Unequal is made to drawing, with both leg sizes and the wall given together. "L profile" on its own cannot be made.
Holes through a leg are sized on bearing, not on tensile. Start with an edge distance of three hole diameters, four is safer, and leave three diameters or more between holes. Glass bearing strength is a fraction of axial tensile, so a narrow edge tears when the bolt is tightened. The inside corner is round, not sharp, with the radius following the wall. A part that has to sit into a square corner needs clearance for that radius, do not draw it against a sharp corner. The junction of the two legs is where the fibre is thickest and where stress concentrates. Keep bolts on the centre line of a leg, away from the junction. For a lengthened run, scarf the joint rather than butting square ends together. A square butt relies entirely on the bolts in shear, which is the weakest direction in glass. A scarf spreads the load into a bonded face and is far steadier. Where metal meets glass, watch galvanic corrosion. The glass itself insulates, so use an insulating washer or matching metals, and do not let stainless steel bite directly into aluminium.
Walkway edge strip, stair nosing, platform edges, anywhere a foot lands, take the grit finish. The grit is embedded in the surface resin during pultrusion, not sprayed on afterwards, so it does not wear off. Grit goes on the outside of one leg only; the other leg stays smooth for bonding. Say at order which leg takes the grit, decided by the leg orientation rather than by which is up. Colour is pigmented into the resin, grey, yellow, green and black are common, and the cut face matches. Grit covers the colour, so grit-finish parts are usually made dark.
Lengths are cut to drawing, the water-jet guided laser cuts to length and drills holes. CNC mills notches, slots and end chamfers, the grit goes on the specified leg. Anything needing sealing is sealed before dispatch. It arrives as a part and goes straight into assembly, cutting. The water-jet guided laser cuts to length and drills holes, with no burning and no breakout, length ±0.1 mm. Sawn to ±2 mm, CNC-milled edge ±0.2 mm, holes and slots. Hole position ±0.01 mm; notches, slots and end chamfers to drawing. Edge distance from three hole diameters, four is safer, glass bearing strength is low, and a short edge tears when the bolt is tightened. Check it at layout, ends. A cut end exposes fibre and water travels along it. Parts for outdoor, damp or chemical service are sealed in house, with resin of the same system or an end cap, threads. The profile is not tapped directly, because interlaminar shear will not hold a thread. Threaded parts take an insert or a through bolt, fitted in house. Glass fibre wears tooling faster than carbon fibre, and both tool consumption and cycle time are higher. That shows up in the machining charge, not in the tolerance. All of this is done on our own profiles only, customer-supplied finished parts are not machined. Customer-supplied fibre or prepreg is processed into product.
| Leg | ±0.5%, minimum ±0.2 mm, maximum ±0.75 mm | The minimum applies to small sections, the percentage to large ones |
|---|---|---|
| Wall, 3 mm band | ±0.20 mm | Thin leg, jointed with through bolts and washers |
| Wall, 5 mm band | ±0.35 mm | The usual load-bearing bracing |
| Wall, 10 mm band | ±0.45 mm | Heavy structure |
| Wall 6 / 8 / 12 mm | 6 mm takes the 5 mm band; 8 mm and 12 mm take the 10 mm band | No separate tolerance between bands |
| Right angle | 90° ±1.5° | Corner capping fit |
| Inside radius | Follows the wall, of the same order | Leave clearance for it on facing parts |
| Straightness | 1.5 mm/m | Accumulates with length on long spans |
| Twist | Leg ≤75 mm: 1.5°/m; >75 mm: 1.0°/m | Wide legs twist more readily |
| Sawn length | +50 / −0 mm | Blank, with machining allowance |
| Water-jet guided laser | ±0.1 mm | Cut-to-length and holes |
| Hole position | ±0.01 mm | To drawing |
| CNC-milled edge | ±0.2 mm | Delivered this way on precision parts |
Load at the edge and a corner to sit into: the angle. Closed on four sides and torsion to resist: box section. For light guardrail and walkway edge strip, an angle uses less material.
Equal for general work: it cannot go on the wrong way round and one stock item covers it. Unequal where one leg bears on a panel and the other carries load — narrow leg as trim. Load at the edge and a corner to sit into: the angle. Closed on four sides and torsion to resist: box section. For light guardrail and walkway edge strip, an angle uses less material
±0.5%, minimum ±0.2 mm, maximum ±0.75 mm
By band: 3 mm band ±0.20, 5 mm band ±0.35, 10 mm band ±0.45, 6 mm takes the 5 mm band. 8 mm and 12 mm take the 10 mm band
90° ±1.5°. Corner capping has to allow for that tolerance — do not draw it to a theoretical square with zero clearance
Round, with the radius following the wall, of the same order. A part going into a square corner needs clearance for that radius at drawing stage
Yes, in house. Hole position ±0.01 mm, edge distance from three hole diameters, and three diameters or more between holes. Slots, notches and chamfers all to drawing
Yes. The grit is embedded in the surface resin during pultrusion and does not wear off. It goes on the specified leg only, so the other leg stays smooth for bonding
Yes. Water-jet guided laser cuts to length and drills holes without burning or breakout: length ±0.1 mm, hole position ±0.01 mm
Yes for outdoor, damp or chemical service, and we seal them in house with resin of the same system or an end cap
Pigmented in the resin — grey, green, yellow and black are common, and the cut face matches, grit-finish parts are usually dark
Yes, both leg sizes and the wall to drawing, with the smallest leg limited by bending. "L profile" alone is not enough; give both legs and the wall
Water-jet guided cutting, CNC milling, drilling, slotting, end chamfers, grit finish and end sealing, all in house. A drawing or a DXF is enough
6 m as standard, and cut to the length you need. Full lengths are the minimum; cut lengths are quoted per piece, and drilled or slotted parts per piece
Section, length, quantity and service conditions — with these in hand the quote is accurate. Upload a drawing if you have one; without one, the same figures written out will do.
A drawing, a photo of a failed part, or three lines of requirement is enough to start. Scope, price indication and lead time within 24 hours.
No commitment · NDA available · Reply within 24 hours