Reference image. The actual surface and colour depend on the resin and the finish.
Overview
A beam that has to cross a distance with no column under it: use an I. The flanges gather the force in, the web carries the shear down, and the material sits at top and bottom. The same weight buys more bending stiffness. It is the most efficient of all the sections, and the price is a weak flank, panel edge to carry and stop. Use a channel rather than an I. Both flanges of an I reach out, so it carries but does not stop, the panel edge can still slide. Edge trim and corner capping: use an angle. Bolts on all four faces and panels flat against the side: use box section, an I does one job: bending. Glass is softer than steel, so at the same section it deflects far more. Selection of an I beam is usually stopped by deflection rather than by strength. Is why the table below gives the second moment of area and not a load capacity: capacity needs a bending strength to go with it. The second moment is pure geometry you can use straight away. An I is stiff on its strong axis and soft on its weak one. The moment the compression flange has no lateral restraint it bends sideways and then twists, and it loses stability well below its bending capacity. This is not a theoretical problem. It is the commonest failure on site: the beam goes in, nothing braces the mid-span, and under load the whole thing rolls over sideways. Where restraint comes from, and how far apart it can be, is set out in the section below. Cut-to-length, holes and slots are all done in house, and a water-jet guided cut goes straight into assembly. An I has thin free flange edges, so keep holes in the web, where one must go in a flange, put it near the root. A drawing or a DXF is enough. If the size you need is not in this table, it becomes a custom composite part.
Grating bearer: Intermediate support for platforms, trench covers and access openings
Walkway stringer: Added under a long platform to break the span
Equipment base beam: Bottom frame under pumps, fans and control cabinets
Frame cross-member: Transverse members in modular structures, racking and guarding frames
Wide-flange bracing: Where depth is limited but lateral resistance is needed — 150×150 and the like
Stock sizes in detail
These section properties hold while the compression flange is restrained laterally. Unrestrained, the beam fails by lateral-torsional buckling well below them — see Lateral stability below.
Depth mm
Flange mm
Wall mm
Section mm²
kg/m
Ixx cm⁴
Iyy cm⁴
Typical use
60
30
4
448
0.90
23.5
1.8
Light frame cross-member
80
40
5
750
1.50
70.6
5.4
Equipment base, small platform
100
50
5
950
1.90
143.3
10.5
Short-span grating beam
100
50
6
1128
2.26
166.8
12.7
Short-span grating beam, heavier load
120
60
6
1368
2.74
297.1
21.8
Walkway stringer
120
70
8
1952
3.90
426.8
46.2
Grating bearer (the usual size)
150
75
8
2272
4.54
766.0
56.8
Platform main beam
150
80
10
2900
5.80
968.4
86.4
Platform main beam, heavier load
150
150
10
4300
8.60
1655.6
563.6
Wide flange, for lateral resistance
200
100
8
3072
6.14
1890.7
134.1
Long-span stringer
200
100
10
3800
7.60
2292.7
168.2
Long-span main beam
200
100
12
4512
9.02
2668.7
202.5
Long span, heavy load
250
125
12
5712
11.42
5406.2
393.9
Large-span main beam
300
150
12
6912
13.82
9571.7
679.0
Large span, heavy load
kg/m is section area × density at 2.0 g/cm³. Section area A = t(2b + h − 2t).
Ixx and Iyy are calculated on a sharp-cornered section, ignoring the inside radius; the radii in a real section make the second moment a little lower than the table, and the smaller the section the bigger the difference. Leave margin when taking a design value, or recompute on the real section.
Ixx is about the strong axis (horizontal), Iyy about the weak axis (vertical), in cm⁴.
Section modulus Wx = Ixx ÷ (h/2), and bending capacity follows M = σ·Wx, with σ taken from your own material strength data.
Main beams, grating bearers, walkway stringers: where an I beam sits An I beam does one thing in a structure: it crosses. A grating platform is the most typical use. L or C runs round as the support edge. An I is laid across at intervals as the bearer, and the grating panel rests on the top flange. The bearer spacing decides how far the grating has to span. Close spacing lets you use thinner grating; wide spacing means heavier grating. The two are decided together, not separately. Walkway stringers are another route. A long platform needs stringers under it to break the span. The top flange takes the deck, the bottom flange carries pipe or trunking, and the web takes holes for services. Web holes go to drawing, with edge distance from three hole diameters. Equipment bases and frame cross-members use I as well. Loads here are concentrated and at fixed positions. Mark where the point loads fall. The same beam behaves very differently with the force at mid-span than at a third point.
Lateral stability: why this beam falls over The strong-axis second moment of an I is several times the weak-axis one, and that ratio is the source of its weakness. Under bending the compression flange wants to move sideways. If the flange is held along its length by grating panels or by a fixed deck, it cannot move. The beam works at the stiffness you calculated. If the flange is free, loads landed on top with nothing fixed, or a deck simply resting there. The compression flange bends sideways first, the section twists with it. Capacity falls off a cliff. Where restraint comes from: <pre>Restraint | Effect
Grating or deck fixed to the top flange (clamp plate, clips, bolts) | Restraint effective
Deck merely resting, free to slide | Restraint not reliable
Bottom flange in tension, usually not the control case | Check supports and end connections
Lateral bracing or knee braces added | Most direct; try spacing at 1/4 to 1/3 of the span</pre> Do not copy a steel beam table. Steel has a higher modulus and different section proportions, so the critical span for lateral stability is not the same as for glass. Calculate it on glass section properties, or work around it with bracing, one brace costs less than a beam a size larger.
Using the second moment: set the deflection, then pick the section The table gives Ixx (strong axis) and Iyy (weak axis). The method is: Set the allowed deflection. Walkways and platforms usually take span/200 or span/300, sometimes a flat 10 mm; equipment bases follow the equipment. That figure is not ours to set, it is the user's. Work out the second moment needed. For a simply supported beam under a uniform load, deflection f = 5wL⁴/(384EI). E is the elastic modulus, taken from your own material data; w is the line load and L the span. Substitute the allowed deflection, solve for the I required, and take the smallest row in the table that is not below it. Then check lateral stability and bearing at the supports. Enough second moment with no restraint still falls over; and if the flange cannot take bearing at the support, the end crushes. Span alone, with no load and no allowed deflection, cannot be selected. All three together and it lands first time.
Division of labour with the channel Both are open sections, and they sit in different places. <pre>I | Pure bending. Main beams, grating bearers, walkway stringers. Both flanges reach out: it carries, it does not stop
C | Bending plus an edge stop. Edge beams, cable tray side rails, grating support edges. One flange carries, one flange stops</pre> On the same platform, C runs round the perimeter as edge beams and I runs through the middle as main beams. The standard arrangement. The two meet at a bracket or a connection plate, with bolts through the web. An I and a C do not substitute for each other. A C used as a main beam has poor torsional resistance and twists at mid-span. An I used as an edge beam will not stop the panel edge without a separate block adding to it.
Post-machining: done in house, arrives as a part Supplied as a full length — 6 m is the standard band, not a maximum — or cut to drawing. <pre>Cutting | Water-jet guided laser for cut-to-length and holes, no burning or breakout, length ±0.1 mm; sawn to ±2 mm
Holes | Hole position ±0.01 mm; holes in a flange as near the root as possible, web holes to drawing
Slots | Notches, slots and end chamfers to drawing, CNC-milled edge ±0.2 mm
Ends | A cut end exposes fibre and water travels along it. Outdoor, damp or chemical service: sealed before dispatch</pre> A flange is a thin free edge, so keep large holes out of it. Where one is unavoidable, put it near the root. The side next to the web, away from the free edge. Glass fibre wears tooling faster than carbon fibre, and both tool consumption and cycle time are higher. That shows up in the machining charge, not in the tolerance. Post-machining is done on our own production only; customer-supplied finished parts are not machined, but customer-supplied fibre or prepreg is processed into product.
Delivery states
Full length Supplied at the standard 6 m, or cut to need, protective film intact
Cut to length Water-jet guided, length ±0.1 mm
Drilled/slotted To drawing, hole position ±0.01 mm
CNC-milled edge Outline and chamfers, ±0.2 mm
Ends Outdoor, damp or chemical service: sealed in house
Assembly Combined with metal parts and inserts, batch after first-article approval
Tolerance and inspection
Depth h
±0.5%, minimum ±0.2 mm, maximum ±0.75 mm
On the nominal size
Flange width b
±0.5%, minimum ±0.2 mm, maximum ±0.75 mm
As above
Wall 4 mm
±0.25 mm
Set by the pultrusion die
Wall 5 mm
±0.35 mm
As above
Wall 6 mm
±0.35 mm
Takes the 5 mm band
Wall 8 mm
±0.45 mm
Takes the 10 mm band
Wall 10 mm
±0.45 mm
As above
Wall 12 mm
±0.45 mm
Takes the 10 mm band
Flange parallelism
0.5 mm / 100 mm
Checked with the pultrusion
Right angle
90° ±1.5°
Flange-to-web squareness, which affects fit
Straightness
1.5 mm/m
Accumulating over the length
Twist
≤150 deep: 1.5°/m; >150 deep: 1.0°/m
Banded by depth
Length (full length)
+50 / −0 mm
End machining allowance
Length (water-jet guided)
±0.1 mm
Delivered this way on precision parts
Hole position
±0.01 mm
To drawing
CNC-milled edge
±0.2 mm
Outline and chamfers
Common questions
I beam or channel, which should I choose?
Look at whether it has to stop an edge. Crossing and bending only, take the I; carrying a panel edge and stopping it as well, take the C. On the same platform, C runs round as edge beams and I runs through as main beams
Can it replace a steel beam directly?
Not by matching the steel section size. Glass is softer than steel, so at the same section it deflects far more. Recalculate on stiffness: set the allowed deflection, solve for the second moment needed, then find the row in the table
Why does the table give the second moment and not a load capacity?
Capacity needs bending strength, span and support conditions together, and changes with every duty. The second moment is pure geometry, usable as it stands, and the customer works deflection out from the formula. Where a capacity calculation is needed, it is issued to drawing as a separate document
Is the second moment measured or calculated?
Calculated on a sharp-cornered section, ignoring the inside radius. A real section has radii, so the second moment is a little lower than the table. The smaller the section the bigger the difference. Leave margin on a design value, or recompute on the real section
Can I leave out bracing at mid-span?
That depends on whether the flange is restrained. Grating or deck fixed to the top flange restrains it; a deck merely resting and free to slide does not count. Without reliable restraint, bracing is obligatory, at spacing tried between 1/4 and 1/3 of the span
Why can't I copy a steel lateral-stability table?
Different stiffness, different section proportions, so the critical span is not the same. Glass has the softer weak axis, so at the same unrestrained length it loses stability sooner, calculate on glass section properties
Can you drill it?
Yes. Web holes to drawing, edge distance from three hole diameters. The flange is a thin free edge, so keep large holes out of it. Where one is needed, put it near the root and away from the free edge.
Can it be laser cut?
Yes, water-jet guided laser. The cut is not blackened and does not chip, length ±0.1 mm. A dry laser will not do it, the resin burns
How long is a full length?
6 m is the standard band rather than a maximum; it can also be cut to drawing
Do the ends need treatment?
Outdoor, damp or chemical service needs sealing. A cut end exposes fibre and water travels along it, so the sealing is done in house
Can you make unequal flanges?
To drawing. Different flange widths top and bottom, or different flange thickness. Both can be made, with the tolerance to drawing.
Can it be tapped?
The profile is not tapped directly. Interlaminar shear will not hold a thread and repeated assembly strips it. Threaded parts take an insert or a through bolt, fitted in house
What is the MOQ?
Full lengths carry an MOQ by product; cut parts are quoted per piece to drawing, samples can be made first
Can it be supplied assembled with metal parts?
Yes. Combined with steel, aluminium or inserts and supplied as an assembly, with the fit confirmed at first-article stage
Send us the size
Section, length, quantity and service conditions — with these in hand the quote is accurate. Upload a drawing if you have one; without one, the same figures written out will do.
Company addressZhuyuan Tianhuan International, No. 76 Keji 2nd Road, High-tech Zone, Xi'an, Shaanxi, China