Overview

A channel does the job of carrying a panel and stopping its edge at the same time. An angle only carries: the panel edge can still slide out. Box section is closed on all four sides, so a carrier strip has to be made and fixed to its side. With a channel the two flanges sit above and below, and a panel dropped between them is held, no separate stop needed. Height 50 to 200 mm, width 25 to 75 mm, wall 3 to 12 mm, commonly in 6 m lengths. Cable tray side rails, grating edge support, platform edge beams, and box and door frame reinforcement all use it this way. It is an open section. Way the opening faces decides how it carries: opening in and opening out differ by a whole band. The section below on the open section works through them. Capacity comes from the height, not from piling on wall thickness. Turn the same profile on its side and the height becomes the width, and capacity drops sharply. Give span, uniformly distributed load and allowed deflection together and the selection lands first time. Cutting, drilling and milling are done in house, and the water-jet guided laser also cuts to length and drills holes. Glass fibre wears tooling faster than carbon fibre, and the extra tool consumption and slower cycle show up in the machining charge. A cut end exposes fibre, so parts for outdoor or damp service are sealed before dispatch. Cut lengths come from here; a machined part comes from custom composite parts.

Request a quote

Where it is used

  • Edge frames and support: cable tray side rails, grating edge support, platform edge beams, walkway edge frames
  • Boxes and door frames: cabinet edging, door frame reinforcement, cover support
  • Cable support: tray side panels, trunking edge support, bracket beams
  • Platforms and access: platform main beams, stair nosing support, trench cover edge beams
  • Chemical and sewage: railing posts, walkway support, equipment base frames

Stock sizes in detail

kg/m is section area × density at 2.0 g/cm³; the section area is given alongside so you can check it.

Height × width mm Wall mm Section mm² kg/m Typical use
50 × 25 3 282 0.56 Light edge support, cover
50 × 25 5 450 0.90 Edge support, box reinforcement
60 × 30 4 448 0.90 Edge frame, cover support
75 × 40 5 725 1.45 Grating edge support
80 × 40 5 750 1.50 Grating edge support, walkway edge frame
100 × 40 5 850 1.70 Platform edge beam
100 × 50 6 1128 2.26 Cable tray side rail
100 × 50 8 1472 2.94 Load-bearing side rail
120 × 50 6 1248 2.50 Cable tray side rail, edge beam
120 × 50 8 1632 3.26 Load-bearing edge beam
150 × 50 6 1428 2.86 Platform edge beam
150 × 75 8 2272 4.54 Main edge beam
150 × 75 10 2800 5.60 Heavy-duty edge beam
200 × 60 8 2432 4.86 Long-span edge beam
200 × 60 10 3000 6.00 Main structural edge beam
200 × 60 12 3552 7.10 Heavy-duty main beam

Edge beam, tray side rail, grating support: where a channel sits

Where a beam has to carry a panel and stop its edge at once, use a channel. The top flange carries, the bottom flange catches, the web between them is the edge stop, and a panel edge goes in without a separate block.

The cable tray side rail is the most typical use of the family: the web holds the cable in, the flange carries the rungs, rung spacing follows span and load, and the side rail height decides how wide the tray can be.

Grating support is the same job: the flange carries the grating, the web stops it moving sideways, and a clamp plate stops it lifting. Give the flange width enough room — too narrow and it will not hold.

Box and door frame reinforcement turns the channel round: it clips over the panel edge and each flange grips a face, so the whole edge is wrapped — the only place on the page where the channel is a wrap rather than a tray. It bends better than an angle and uses less material than box section.

Open section: which way the opening faces

A channel is singly symmetric, and the open side is the soft one. Opening in or opening out changes torsional resistance by a whole band.

Opening in, with the panel inside it, is the commonest. The flanges are in compression, the panel props the opening, and the section comes close to closed — the strongest posture a channel has.

Opening out, web against the structure, passes bolts through the web and is the easiest to install. The cost is that both flange free edges are exposed, so torsion and flange local buckling have to be checked separately; on a long span or with eccentric load, add bracing or a diaphragm.

Height is the working direction. Turn the same channel on its side and the height becomes the width, and capacity drops sharply — not an estimate, but the major axis rotating 90°.

Joints: the web takes shear, the flanges take bending

The web is the main shear face. Bolts, self-tapping screws and blind rivets all go on the web centre line, with edge distance from three hole diameters, four safer, and three diameters or more between holes.

The flange is a thin free edge, so keep large holes out of it. Where one is unavoidable, put it near the root — close to the web, away from the free edge; the larger the hole, the closer to the root.

Two lengths joined end to end should not rely on the end faces alone. Add a splice plate inside, or sleeve a length of the same channel over the joint, so the load passes through the web; an open section butted end to end relies almost entirely on bolts in shear, which is the weakest direction in glass.

Long spans need a diaphragm or bracing. A channel has low torsional stiffness, and without mid-span restraint the compression flange buckles first.

Where metal meets glass, watch galvanic corrosion. The glass itself insulates, so use an insulating washer or matching metals, and do not let stainless steel bite directly into aluminium.

Tray and grating: which dimensions the system fixes

Cable tray: side rail height from span and cable load, width from rung length, rung spacing from load and allowed deflection. Side rail and rungs are bolted through the web, hole positions to the system drawing.

Grating: the flange has to take the grating thickness plus the clamp plate, generally not below 40 mm; at a corner, mitre the same channel to 45° or use a corner bracket.

Platform edge beam: height is set by span, uniformly distributed load and allowed deflection together — not by what someone else used. Give all three and the selection is right first time.

Post-machining: done in house, arrives as a part

Lengths are cut to drawing, the water-jet guided laser cuts to length and drills holes, CNC mills notches, slots, 45° mitre cuts and end chamfers, and anything needing sealing is sealed before dispatch. It arrives as a part and goes straight into assembly.

Cutting: water-jet guided laser for cut-to-length and holes, no burning and no breakout, length ±0.1 mm; sawn to ±2 mm, CNC-milled edge ±0.2 mm.

Holes and slots: hole position ±0.01 mm; notches, slots and end chamfers to drawing. Edge distance from three hole diameters, four is safer — glass bearing strength is low, and a short edge tears when the bolt is tightened, so check it at layout.

Ends: a cut end exposes fibre and water travels along it. Parts for outdoor, damp or chemical service are sealed in house, with resin of the same system or an end cap.

Threads: the profile is not tapped directly, because interlaminar shear will not hold a thread. Threaded parts take an insert or a through bolt, fitted in house.

Glass fibre wears tooling faster than carbon fibre, and both tool consumption and cycle time are higher; that shows up in the machining charge, not in the tolerance.

All of this is done on our own profiles only; customer-supplied finished parts are not machined, but customer-supplied fibre or prepreg is processed into product.

Delivery states

  • Full length Supplied at standard length, protective film intact
  • Cut to length Cut to drawing, ±2 mm
  • Laser cut Water-jet guided laser for cut-to-length and holes, ±0.1 mm
  • Precision cut CNC-milled edge and 45° cuts, ±0.2 mm
  • Drilled and slotted To drawing, hole position ±0.01 mm
  • Ends Sawn edge / CNC chamfer / sealed end
  • Grit finish Anti-slip grit on the specified flange face, supplied with the batch
  • Assembly Combined with metal parts and inserts, batch after first-article approval

Tolerance and inspection

Height and width ±0.5%, minimum ±0.2 mm, maximum ±0.75 mm The minimum applies to small sections, the percentage to large ones
Wall, 3 mm band ±0.20 mm Thin wall; joint with through bolts and washers
Wall, 5 mm band ±0.35 mm The usual edge support and edge beam
Wall, 10 mm band ±0.45 mm Heavy structure
Wall 6 / 8 / 12 mm 6 mm takes the 5 mm band, 8 and 12 mm take the 10 mm band No separate tolerance between bands
Right angle 90° ±1.5° Flange-to-web squareness, which affects fit
Straightness 1.5 mm/m Accumulates with length on long spans
Twist Height ≤100 mm: 1.5°/m; >100 mm: 1.0°/m Open sections twist more readily
Sawn length +50 / −0 mm Blank, with machining allowance
Water-jet guided laser ±0.1 mm Cut-to-length and holes
Hole position ±0.01 mm To drawing
CNC-milled edge ±0.2 mm Delivered this way on precision parts

Common questions

Channel or angle, which should I choose?

Carry only, take the angle. Carry and stop the panel edge, take the channel: two flanges hold the edge so it cannot slide out. An angle needs a separate stop added. For a beam that only has to cross a span, with nothing at the edge to stop. An I beam does the same job for less material, see GRP I beam. Channel or box section

Which should I choose?

Box section is closed and resists torsion, but its sides are flat, so carrying a panel means making up a carrier strip. A channel opens upwards or inwards and solves both jobs at once, with less material. Height or width

Height or width, which is the working direction?

Height. Capacity depends mainly on height; width only decides how wide a panel the flange can carry. Turn the same channel on its side and capacity drops sharply. Height. Capacity depends mainly on height; width only decides how wide a panel the flange can carry. Turn the same channel on its side and capacity drops sharply

Opening in or opening out?

Opening in, with the panel inside, is the commonest: flanges in compression and the opening propped. Opening out is easier to install, but both free edges are exposed, torsional resistance is weaker, and a long span needs bracing

What is the height tolerance?

Height and width are both ±0.5%, minimum ±0.2 mm, maximum ±0.75 mm

What is the wall tolerance?

By band: 3 mm band ±0.20, 5 mm band ±0.35, 10 mm band ±0.45. 6 mm takes the 5 mm band, 8 and 12 mm take the 10 mm band

How accurate is the inside width?

It is set by the die and inspected to drawing. It has to mate with an existing part. Give the inside width and the mating part dimensions together and we check them against the drawing

Can I drill the flange?

Yes, but keep the hole near the root and away from the free edge, the flange is thin. A hole near the free edge tears when the bolt is tightened. The web is the safest place for holes

Can it be laser cut?

Yes. Water-jet guided laser cuts to length and drills holes without burning or breakout: length ±0.1 mm, hole position ±0.01 mm

How do I join two lengths?

Not end face to end face. Add a splice plate or sleeve a length of the same channel over the joint so the load passes through the web. Stagger the holes at the joint

Can you do 45° mitres?

Yes, CNC cuts the 45° mitre, and two lengths make a right-angled frame, mitre tolerance ±0.2 mm

Can I choose the colour?

Pigmented in the resin, grey, green, yellow and black are common, and the cut face matches, grit-finish parts are usually dark

What is the MOQ?

Full lengths are the minimum; cut lengths are quoted per piece, and drilled or slotted parts per piece

Send us the size

Section, length, quantity and service conditions — with these in hand the quote is accurate. Upload a drawing if you have one; without one, the same figures written out will do.

No file selected

PDF, DWG, DXF, STEP, STL, ZIP or a phone photo — up to 20 MB.

The part, the material, the size — or the problem it has to solve. Drawings and photos can go in the field above.

+ Company, quantity, timeline

Used only to answer this enquiry and for related technical follow-up.

  • Company address Zhuyuan Tianhuan International, No. 76 Keji 2nd Road, High-tech Zone, Xi'an, Shaanxi, China
  • Factory Fengjing Industrial Park, Middle Section of Fengwu East Road, Huyi District, Xi'an, Shaanxi, China
  • Sales email sales@atomfrp.com
  • Phone (WeChat) +86 18191567691 Email and forms answered 24/7; phone Mon–Fri 09:00–18:00 GMT+8
  • WhatsApp +853 68617664 Email and forms answered 24/7; phone Mon–Fri 09:00–18:00 GMT+8
  • A named engineer replies within 24 hours
  • NDA can be signed before any file is sent
  • Drawings and requirements are not disclosed

Send the drawing. We will send the route.

A drawing, a photo of a failed part, or three lines of requirement is enough to start. Scope, price indication and lead time within 24 hours.

No commitment · NDA available · Reply within 24 hours

Request a quote WhatsApp