Glass fibre rod or carbon fibre rod, how do I choose?
Two questions: insulation, and torsion, need insulation, glass fibre. Need torque resistance, or extreme light-and-stiff, carbon fibre, the price differs several times over
Reference image. The actual surface and colour depend on the resin and the finish.
For bending strength at low weight, choose a tube. For crush resistance, shear, drilling, pinning or being clamped, choose a solid rod. It has no sidewall that can collapse. Putting a tube where a rod belongs is usually not a strength failure but a local crush: a clamp flattens it. A pin hole cracks under load. Cut lengths come from here. A machined part comes from custom composite parts.
Normal batches ship in 15–20 calendar days from drawing approval and receipt of deposit.
| Diameter mm | Tolerance | Usual length | Process | Typical use |
|---|---|---|---|---|
| 3–10 | ±0.15 mm | 1 / 2 m | pultruded | cable racks, guardrail posts, low-voltage insulating rods |
| over 10 to 50 | ±0.20 mm | 2 / 3 m | pultruded | structural supports, equipment posts, live-line operating rods |
| over 50 to 150 | ±0.30 mm | 3 / 6 m | pultruded | large-diameter supports, ladder rails |
| 3–50 ground | ±0.05 mm | to drawing | pultruded + ground | pins, guide rails, parts with a fit requirement |
Sizes outside the table are made to drawing.
| Diameter | ±0.15 / ±0.20 / ±0.30 mm | Micrometer, by band |
|---|---|---|
| Diameter (ground) | ±0.05 mm | Micrometer after grinding |
| Length up to 2 m | ±0.1 mm | At 20 °C |
| Length over 2 m | ±0.5 mm | At 20 °C |
| Straightness | 1 mm/m | Dial gauge on a surface plate |
Two questions: insulation, and torsion, need insulation, glass fibre. Need torque resistance, or extreme light-and-stiff, carbon fibre, the price differs several times over
Banded as in the table; grinding gets it to ±0.05 mm (quoted separately). For parts with a fit requirement, put the tolerance on the drawing. We quote to the drawing, not to a catalogue item
Yes, cutting is in-house and the ends are sealed after cutting. Length tolerance is ±0.1 mm up to 2 m and ±0.5 mm over 2 m, both measured at 20 °C
The fibre does not mind sun; the resin does. UV chalks the resin and water absorption degrades performance. The answer is the right resin and proper surface and end sealing rather than a bigger diameter
Yes. Natural, yellow and black are the three we run routinely. Other colours are matched to a colour card, with MOQ and lead time quoted separately
Section, length, quantity and service conditions — with these in hand the quote is accurate. Upload a drawing if you have one; without one, the same figures written out will do.
A drawing, a photo of a failed part, or three lines of requirement is enough to start. Scope, price indication and lead time within 24 hours.
No commitment · NDA available · Reply within 24 hours